AN ELECTRON DIFFRACTION ANALYSIS OF PRECIPITATES IN A 13Ni MARAGING STEEL (280kgf/mm~2)
Li Douxing and Ye Hengqiang (Institute of Metal Research; Academia Sinica)
Cite this article: 

Li Douxing and Ye Hengqiang (Institute of Metal Research; Academia Sinica). AN ELECTRON DIFFRACTION ANALYSIS OF PRECIPITATES IN A 13Ni MARAGING STEEL (280kgf/mm~2). Acta Metall Sin, 1981, 17(6): 625-634.

Download:  PDF(2609KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The precipitates in 13Ni maraging steel (280 kgf/mm~2) have been identified in relation to the orientation of σ and δ phases in martensite matrix by means of X-ray and selected area electron diffraction analyses. It was shown that the precipitates as an intermetallie compound of δ-(Fe,Ni,Co)Mo are responsible for strengthening in the steel. In case as-forged after aging, μ-phase appeared may reduce its toughness. After over-aging, e. g. 580℃ for 16h, a. c., some reverted austenite was formed. From observation in situ on heating the aged specimen in electron microscope up to 743℃, the δ grains were coalesced and the needle-like σ phase precipitated. Though the diffraction patterns of δ or σ phase can be commonly indexed, the difference of orientation between δ/α and σ/α seems to be more easily used to distinguish them in the maraging steel.
Received:  18 June 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I6/625

[1] Magnee, A., Viatour, P., Drapier, J. M., Coutsouradis, D. and Habraken, L., Cobalt, (1973) , No 1, 3.
[2] Drapier, J. M., Viatour, P., Masnee, A. C. and Coutsouradis, D., Cobalt, (1971) , No. 50,29.
[3] 河部義邦,中沢興三,宗木政一,铁钢,62(1976) ,1229.
[4] 金属研究所,资料.
[5] Kitchingman, W. J., Acta Cryst., A24 (2) (1968) , 282.
[6] Mourey, M., Bui, N. and Dabosi, F., Mater. Res. Bull., 10 (1975) , 565.
[7] 金属研究所,内部资料.
[8] Shocmakcr, C. B., Fox, A. H. and Shoemaker, D. P., Acta Cryst., 13 (1960) , 585.r
No related articles found!
No Suggested Reading articles found!