Please wait a minute...
Acta Metall Sin  1981, Vol. 17 Issue (4): 467-477    DOI:
Current Issue | Archive | Adv Search |
EVALUATION OF BRITTLE-FRACTURE SURFACE ENERGY IN CUBIC METALS BY LATTICE DYNAMICAL METHOD
by Sun Xiaokai; Xiong Liangyue and Long Qiwei (Lung Chi-wei)(Institute of Metal Research; Academia Sinica)
Cite this article: 

by Sun Xiaokai; Xiong Liangyue and Long Qiwei (Lung Chi-wei)(Institute of Metal Research; Academia Sinica). EVALUATION OF BRITTLE-FRACTURE SURFACE ENERGY IN CUBIC METALS BY LATTICE DYNAMICAL METHOD. Acta Metall Sin, 1981, 17(4): 467-477.

Download:  PDF(721KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Using the method of linear response theory in lattice dynamics on the basis of Tyson's model, the response displacements of atoms on cleavage plane at the incipience of brittle fracture was derived and an expression for evaluating brittle fracture surface energy of metals was found. The brittle fracture surface energy for a number of bcc and fcc metals has been calculated and the results coincide with order of magnitude in experimental measurements.
Received:  18 April 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I4/467

[1] 龙期威,中国物理学会年会上的报告,1978年8月庐山.龙期威,全国断裂物理与断裂力学学术讨论会(武汉)文集,1978年10月.
[2] Caglioti, G., Rizzi, G. and Bilello, J. C., J. Appl. Phys., 42 (1971) , 4271; J. Appl. Phys. 43 (1972) , 3600.
[3] Tyson, W. R., J. Appl. Phys., 47 (1976) , 459.
[4] Kwok, P. C. K., Solid State Phys., 20 (1967) , 213.
[5] Boffi, S., Proc. Int. School Phys. Enrico Fermi Course LXI Ed. by G. Caglioti, North-Holland New York, 1976, p. 315.
[6] Gilman, J. J., Fracture of Solid, Ed. by D. C. Drucker and J. J. Gilman, New York, 1963, p. 541.
[7] A.塞格,晶体的范性及其理论,张宏图译,科学出版社,1963.
[8] Jones, H. and Leak, G. M., Metal Sci. J., 1 (1967) , 211.m
No related articles found!
No Suggested Reading articles found!