Please wait a minute...
Acta Metall Sin  1981, Vol. 17 Issue (4): 461-466    DOI:
Current Issue | Archive | Adv Search |
A BOND PARAMETER APPROACH TOW ETTABILITY OF MOLTEN GLASS ON Pt ALLOY
by Ning Yuantao; Wang Yongli(Institute of Precious Metals)and Yuan Qilong (Nanjing Institute of Glassfibre)
Cite this article: 

by Ning Yuantao; Wang Yongli(Institute of Precious Metals)and Yuan Qilong (Nanjing Institute of Glassfibre). A BOND PARAMETER APPROACH TOW ETTABILITY OF MOLTEN GLASS ON Pt ALLOY. Acta Metall Sin, 1981, 17(4): 461-466.

Download:  PDF(489KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The bond parameter approach to the wetting behaviour of molten glass on certain Pt alloys was attempted on the basis of their equilibrium contact angle tests. It seems to indicate that the dependence of the wetting behaviour on the bond parameters of pure metals, and Pt-alloy constituents as well as glass components itself may be qualitatively generalized.
Received:  18 April 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I4/461

[1] Copley, G. J., Rivers, A. D. and Smith, R., J. Mater. Sci., 10 (1975) , 1285.
[2] Selman, G. L., Spender, M. R. and Darling, A. S., Platinum Met. Rev. 9 (1965) . 130.
[3] Copley, G. J. and Rivers, A. D., J. Mater. Sci., 10(1975) , 1291.
[4] Zackay, V. F., Mitchell, D. W., Mitoff, S. P. and Pask, J. A., J. Am. Ceram. Soc., 36 (1953) , 84.
[5] Fulrath, R. M., Mitoff, S. P. and Pask, J. P., J. Am. Ceram. Soc., 40 (1957) , 269; 118.
[6] Volpe, M. L., Fulrath, R. M. and Pask, J. A., J. Am. Ceram. Soc., 42 (1959) , 102.
[7] #12
[8] 陈念贻,键参数函数及其应用,科学出版社,1976,p.74.
[9] #12