Acta Metall Sin  1981, Vol. 17 Issue (3): 233-242    DOI:
Current Issue | Archive | Adv Search |
EFFECTS OF RARE EARTH ON PREFERRED ORIENTATION IN OXIDE SCALE O FA Fe-Cr-Al ALLOY
by Zhang Lixin; Luo Jixun; Yin Yaode and Li Liguang (Institute of Metal Research; Academia Sinica) Zhao Qi and Zhang Jiayun
Cite this article: 

by Zhang Lixin; Luo Jixun; Yin Yaode and Li Liguang (Institute of Metal Research; Academia Sinica) Zhao Qi and Zhang Jiayun. EFFECTS OF RARE EARTH ON PREFERRED ORIENTATION IN OXIDE SCALE O FA Fe-Cr-Al ALLOY. Acta Metall Sin, 1981, 17(3): 233-242.

Download:  PDF(820KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effects of RE additions, 0.5% Y or 0.15% (La+Ce), on the prefe ed orientation of oxide scale formed at 1200℃ in a Fe-Cr-Al alloy have been studied by inverse-pole-figure method. It was found that the addition of RE element affects the types of preferred orientation to a limited extent.The main preferred orientation in the oxide scale on three tested alloys are identical as (0118);whereas some differences are shown among their minor ones with (1129)and (10110) for alloys containing Y or La+Ce, and (0001) and (10110) for an alloy without RE. RE can play an important part in conserving and enhancing the preferred orientations in the scale, among which Y has a more remarkable effect than La+Ce.The oxidation process of the alloys was discribed by the shortcircuit dislocation path model. This model makes the variation curve of P_1011 parameter of the oxide scale in good agreement with the variation curves of oxidation dynamics. This accounts for the fact that RE elements improve the oxidation resistance of the alloy through their effect on modifying the preferred orientation of the oxide scale.
Received:  18 March 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I3/233

[1] 骆继勋、银耀德、林生昆、赵齐、王俭,金属学报,13(1977) ,263.
[2] 天野忠昭,矢島聖使,斎藤安俊,日本金属学会誌,41(1977) ,1074.
[3] Golightly, F. A., Sott, F. H. and Wood, G. C., Oxid. Metals, 10 (1976) , 163.
[4] Kubaschewski, O. and Hopkins, B. E., Oxidation of Metals and Alloys, 2nd ed. Butterworths, London, 1962, p. 66.
[5] Muller, M. H. Chernock, W. P. and Beck, P. A., Trans. AIME, 212 (1958) , 39.
[6] Klug, H. P. and Alexander, L. E., X-Ray Diffraction Procedures for Polycrystalline and Amorphous, 2nd ed., John Wiley & Sons New York, 1974, p. 360.
[7] 张立新、银耀德、李黎光、赵齐、张丙申,金属学报,16(1980) .
[8] Felten, E. J. and Pettit, F. S., Oxid. Metals, 10 (1976) , 189.
[9] Hirota, K. and Komatsu, W., J. Amer. Ceram. Soc., 60 (1977) , 105.
[10] Sadananda, K. and Marcinkowski, M. J., J. Appl. Phys., 45 (1974) , 1521.
[11] Stephens, D. L. and Alford, W. J., J. Amer. Ceram. Soc., 47 (1964) , 81.
[12] Scheuplein, R. and Gibbs, P., J. Amer. Ceram. Soc., 43 (1960) , 458.
No related articles found!
No Suggested Reading articles found!