Please wait a minute...
Acta Metall Sin  1981, Vol. 17 Issue (3): 243-364    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF Al ON THE MAGNETIC PROPERTIES OF GRAIN-ORIENTED 3%Si-Fe
by Luo Yang; Li Weili; Li Yufeng; Chen Yizhi and Chen Minqin (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry)
Cite this article: 

by Luo Yang; Li Weili; Li Yufeng; Chen Yizhi and Chen Minqin (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry). EFFECT OF Al ON THE MAGNETIC PROPERTIES OF GRAIN-ORIENTED 3%Si-Fe. Acta Metall Sin, 1981, 17(3): 243-364.

Download:  PDF(4197KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Studies were made of the effect of A1 on the magnetic properties of grainoriented 3%Si-Fe containing about 0.007 wt-% N and 0.001—0.0088 wt-% A1. The nitrogen content, both soluted and combined in steels were determined by hydrogen extracting method. It is shown that every optimum range of A1 content in steels is available to its own soaking temperature for the purpose of obtaining proper magnetic properties as B_(10)≥1.8T and P15/50≤1.05W/kg, such as 0.008—0.018, 0.005—0.022, 0.004—0.03 and 0.05 wt-% A1 correspond 1200, 1250, 1300 and 1350℃ respectively. If any A1 content was beyond the optimum range, their magnetic properties would be steeply fallen to such extent even as a value of the non-oriented steel. It is also found that the A1 content influences markedly upon the proportion of A1N which is an effective inhibitor to normal grain growth.Most effective A1N may be precipitated while the acid soluble A1 is within 0.005—0.02%. Owing to the aforementioned results together with that of electron microscope observation and thermodynamical consideration of A1N and MnS, an approach about the behaviour of A1 on magnetic properties of grain-oriented 3%Si-Fe was proposed, namely, the Al is associated with N to form AlN, and then A1N exists as an effective inhibitor.
Received:  18 March 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I3/243

[1] 罗阳、陈易之、张百成、马黛,金属学报,13(1977) ,80.
[2] Littmann, M. F., Met. Trans., 6A (1975) , 1041.
[3] Wriedt, H. A. and Hu, H., Met. Trans. 7A (1976) , 711.
[4] Iwayama, K. and Haratani, T., J. Magn. Magn. Mater., (1980) , 15.
[5] 罗阳、张百成、周秀媛、马鸿良,金属学报,16(1980) ,38.
[6] Oelsen, W. und Sauer, K.-H., Arch. Eisenhuettenw., 38 (1967) , 141.
[7] 陈名浩、张代仁,氢抽取法测定硅钢中固氮气和有效粒度氮化铝,1979(待发表)
[8] Sakai, T., Shiozaki, M., and Takashina, K., J. Appl. Phys., 50 (1979) , 2369.
[9] Kumai, K., Motoyoshi, M., Tanaka, K. and Hakiwara, Y., U. S. Pat. № 3 671 337, 1973.
[10] #12
No related articles found!
No Suggested Reading articles found!