| A STUDY ON THE DEFORMATION AND PRIMARY RECRYSTALLIZATION TEXTURE IN A MnS-AlN-INHIBITED 3% SILICON STEEL |
| Lü Qichun; Shuai Renjie; Zhou Xiuyuan and Zhao Xizhen (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry) |
|
Cite this article:
Lü Qichun; Shuai Renjie; Zhou Xiuyuan and Zhao Xizhen (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry). A STUDY ON THE DEFORMATION AND PRIMARY RECRYSTALLIZATION TEXTURE IN A MnS-AlN-INHIBITED 3% SILICON STEEL. Acta Metall Sin, 1981, 17(1): 58-127.
|
|
|
Abstract The deformation and primary recrystallization texture in a MnS-AlN-inhibited 3%Si steel has been investigated by X-ray diffraction and etching pits technique. Differing from the convcntional grain oriented silicon steel, the hot rolling texture of the MnS-AlN-inhibitcd 3%Si steel consists mainly of {112}<110>, {111}<110>, {100}<110> and {111}<112> components. The cold roiling textures were found to be correlated with the hot rolling textures by inheritance as the cold reduction percentage is within the range of 80—87%, and changed toward thestable {100}<011> orientation when it is over 87%. Apparently, this latter case is unfavourable to the magnetic properties of the steel. The correlation between the transformations of hot rolling, cold rolling and primary rccrystallization textures has also been discussed.
|
|
Received: 18 January 1981
|
[1] 田口悟,日本金属学会会报,13(1974) ,49. [2] 的场伊三夫,川崎制缺技报,1975,№ 4,175. [3] Dunn, C. G., Acta Met., 2 (1954) , 173. [4] Dunn, C. G. and Koh, P. K., Trans. AIME, 209 (1957) , 81. [5] #12 [6] #12 [7] #12 [8] Datta, A..IEEE Trans. Magn., Mag-12 (1976) , № 6, 1. [9] 松岡孝,铁钢,52(1966) ,1179. [10] Mobius.H. E. und Pawlek, F., Arch Eisenhuettenw., 29(1958) , 423. [11] 阿部秀夫,日本金属学会誌,29(1965) ,1221. [12] Hu, H.,Recovery and Recrystallization of Metals,Proceedings of a Symposium Held in New York, N. Y.,Feb.1962, ed. by L.Himmel, Wiley, New York, 1963, p. 311. [13] Dillamore, I. L.,Trans. AIME, 233(1965) , 702. [14] Dunn, C. G. and Koh, P. K., Trans. AIME, 206 (1956) , 1017. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|