Please wait a minute...
Acta Metall Sin  1981, Vol. 17 Issue (1): 67-72    DOI:
Current Issue | Archive | Adv Search |
THERMAL EXPANSION ANOMALIES OF THE COMPOUNDS RECo_5
Yang Yingchang; Ho Wenwang and Lin Qin (Belling University)
Cite this article: 

Yang Yingchang; Ho Wenwang and Lin Qin (Belling University). THERMAL EXPANSION ANOMALIES OF THE COMPOUNDS RECo_5. Acta Metall Sin, 1981, 17(1): 67-72.

Download:  PDF(439KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The temperature dependence of the lattice constants of the compounds CeCo_5, Ce (Co_(0.8) Cu_(0.2))_5 and Ce (Co_(0.9) Fe_(0.1))_5 in the range from room temperature to 600℃ has been studied. CeCo_5 shows an invar-type thermal expansion anomalies in axis c below the Curie temperature. But the anomalies are considerably reduced on the partial substitution of the Co atoms by the Cu atoms. Studies of the neutrons diffraction have been carried out on the compounds Y (Co_(0.8) Cu_(0.2))5, and it has been found that the Cu atoms prefer to occupy the site 2c. There by the thermal expansion anomalies along axis c of the compounds RECo_5 is explained.
Received:  18 January 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I1/67

[1] Jennings, L. D. and Chipman, D. R., Amer. Inst. Phys. Conf. Proc., № 18, 1973, p. 1187.
[2] Buschow, K. H. J,, Miedema, A. R. and Brouha, M., J. Less-Common Metals, 38 (1974) , 9.
[3] 孙天铎、祝景汉、王德文,金属学报,15(1979) ,58.
[4] Neel, L., Ann. Phys.,5(1936) , 232.
[5] Yang,Y.T.(杨应昌),Ho,W.W.(何文望),Yang,L.K.(杨继廉)Tchou,T.S.(朱家瑄), Tseng,S.S.(曾祥欣)et Kin,L.(金兰),J.Phys.,Colloq. C5, Supplement au N°5,Tome 40,Mai 1979,p.C5-117.
No related articles found!