AN ELECTRON MICROSCOPE OBSERVATION OF INTERPHASE CARBIDE PRECIPITATION IN 10MoWVNb
Chen Mengzhe; Li Huarui and Cheng Guijuan (Belling University of Iron and Steel Technology) and Ge Mohui (Shanghai № 1 Steel Works)
Cite this article: 

Chen Mengzhe; Li Huarui and Cheng Guijuan (Belling University of Iron and Steel Technology) and Ge Mohui (Shanghai № 1 Steel Works). AN ELECTRON MICROSCOPE OBSERVATION OF INTERPHASE CARBIDE PRECIPITATION IN 10MoWVNb. Acta Metall Sin, 1981, 17(1): 103-132.

Download:  PDF(1601KB) 
Export:  BibTeX | EndNote (RIS)      
Received:  18 January 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I1/103

[1] Davenport, A. T., Berry, F.G. and Honeycombe, R. W. K., Metal Sci. J., 2 (1968) , 104.
[2] Gray, J. M. and Yeo, R. B. G., ASM Trans. Quart., 61 (1968) , 255.
[3] Davenport, A. T. and Honeycombe, R. W. K., Proc. Roy. Soc., 322A (1971) , 191.
[4] Honeycombe, R. W. K., Trans. AIME, 7A (1976) , 915.
[5] Honeycombe, R. W. K., Scand. J. Met., 8 (1979) , 21.
[6] Purdy, G. R., Acta Met., 26 (1978) , 487.
[7] 陈梦谪,李华瑞,程桂娟,葛默辉,北京钢铁学院学报,1979,№ 2,150.
[8] 葛默辉,陈梦谪,李华瑞,程桂娟,内部资料,1979
No related articles found!
No Suggested Reading articles found!