AN IN SITU OBSERVATION OF DEFORMATION AND FRACTURE PROCESS IN METAL PART Ⅱ CLEAVAGE PROCESS IN Nb-W-Zr
Xu Yongbo; Liu Mingzhi; Yu Zhang and Zhu Guiqiu (Institute of Metal Research; Academia Sinica)
Cite this article:
Xu Yongbo; Liu Mingzhi; Yu Zhang and Zhu Guiqiu (Institute of Metal Research; Academia Sinica). AN IN SITU OBSERVATION OF DEFORMATION AND FRACTURE PROCESS IN METAL PART Ⅱ CLEAVAGE PROCESS IN Nb-W-Zr. Acta Metall Sin, 1981, 17(1): 101-130.