DETERMINATION OF DIFFUSION COEFFICIENT OF CARBON IN LIQUID IRON
Han Qiyong;Han Tongfu;Wang Jian Beijing Institute of Iron and Steel Technology
Cite this article: 

Han Qiyong;Han Tongfu;Wang Jian Beijing Institute of Iron and Steel Technology. DETERMINATION OF DIFFUSION COEFFICIENT OF CARBON IN LIQUID IRON. Acta Metall Sin, 1980, 16(4): 435-441.

Download:  PDF(944KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The diffusion coefficient of carbon in liquid iron has been determined byrotating disk method in the temperature range of 1550--1680℃ under argonatmosphere, the temperature dependence of diffusion coefficient being D=4.76 exp(-38000/RT). It was shown that in the case of either complete deoxidation orwithout any deoxidation, the reaction between solid carbon and liquid iron usu-ally lies in the region of diffusion kinetics. In the former case, the diffusion ofcarbon is the rate controlling factor of the reaction. While in the latter case, theoverall reaction consists of two parallel processes-the solution of carbon andthe reaction of solid carbon with the oxygen in liquid iron. The reaction rate isthen controlled by the diffusion of both carbon and oxygen.
Received:  18 April 1980     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1980/V16/I4/435

[1] #12
[2] #12
[3] #12
[4] #12
[5] #12
[6] #12
[7] #12
[8] #12
[9] #12
[10] Elliott, J. F. The Physical Chemistry of Steelmaking, ed. J. F. Elliott, Wiley, New York, 1958. p. 37.
[11] 北京钢铁学院物化教研室同位素研究组,金属学报,13(1977) ,202.
[12] Barfield, R. N. and Kitchener, J. A., J. Iron Steel Inst., 180 (1955) , 324.
[13] Chipman, J., Alfred, R. M., Gott, L. W., Small, R. B., Wilson, D. M., et al, Trans. Amer. Soc. Metals, 44(1952) , 1215.
[14] Yang Ling (杨琳), and Derge, G., Physical Chemistry of Process Metallurgy, Ed. by George R. St. Pierre, 1961, Vol. 7, Pt. Ⅰ, p. 503.
[15] Hume-Rothery, W., J. Iron Steel Inst., 188 (1958) , 113.
[16] #12
[17] #12
[18] Dayal, P. and Darken, L. S., Trans AIME, 188 (1950) , 1156.
[19] #12
[20] #12
[21] #12
[22] #12
[23] Schwerdtfeger, K., Trans AIME, 239 (1967) , 134.
[24] Oberg, K. E., Friedman, L. M., Szwarc, R., Boorstein, W. M. and Rapp, R. A., J. Iron Steel Inst. 210 (1972) , 359.