ON THE WETTABILITY OF CARBON ELECTRODES BY MOLTEN CRYOLITE-ALUMINA ELECTROLYTE
Qiu Zhuxian and Wei Chingbin
Cite this article: 

Qiu Zhuxian and Wei Chingbin. ON THE WETTABILITY OF CARBON ELECTRODES BY MOLTEN CRYOLITE-ALUMINA ELECTROLYTE. Acta Metall Sin, 1980, 16(3): 357-361.