    					| MICROSCOPIC IDENTIFICATION OF AIN | 
  					 
  					  										
						| Zhang Detang | 
					 
															
						 | 
					 
				 
				
				Cite this article: 
				
					
			      Zhang Detang. MICROSCOPIC IDENTIFICATION OF AIN. Acta Metall Sin, 1980, 16(3): 354-382.	
				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
              
				
												  
													
													    | 
													    	
														 | 
													 
																										
													
														| 
															
													     		                            						                            																	    Abstract  A microscopic observation on AIN phase is made together with EPMA, X-rayor electron diffraction analysis. Its crystalline structure as well as chemical andmechanical properties are presented, and its original colour or optical feature isshown in colour photos.
																										     | 
														 
												  		
														
															| 
															    																	Received:  18 March 1980
																	    
															    															    															  
															 | 
															
														 
														 																											    																											 
												 
												
												
												
												 
												
												  
             
                         
            
									            
									               
																												  