Acta Metall Sin  1980, Vol. 16 Issue (3): 336-378    DOI:
Current Issue | Archive | Adv Search |
AN ETCH METHOD OF REVEALING CARBIDES IN W CONTAINING ALLOY CAST IRON
Jiang Xiaoxia Institute of Metal Research; Academia Sinica
Cite this article: 

Jiang Xiaoxia Institute of Metal Research; Academia Sinica. AN ETCH METHOD OF REVEALING CARBIDES IN W CONTAINING ALLOY CAST IRON. Acta Metall Sin, 1980, 16(3): 336-378.

Download:  PDF(1292KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The electrochemical behaviour of the carbides in W containing alloy cast ironhas been investigated in the basic solution. As a result, the potentiostatic electro-lytic and chemical etch method for differentially revealing various carbids in thisalloy is proposed.
Received:  18 March 1980     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1980/V16/I3/336

No related articles found!
No Suggested Reading articles found!