Please wait a minute...
Acta Metall Sin  1980, Vol. 16 Issue (3): 331-377    DOI:
Current Issue | Archive | Adv Search |
SOME FACTORS AFFECTING THE WELDED JOINT FRACTURE IN HOT-ROLLED SILICON STEEL COIL
Qi Lian;Pu Shaokang;Yin Biqun Research Institute of Wuhan Iron and Steel Company
Cite this article: 

Qi Lian;Pu Shaokang;Yin Biqun Research Institute of Wuhan Iron and Steel Company. SOME FACTORS AFFECTING THE WELDED JOINT FRACTURE IN HOT-ROLLED SILICON STEEL COIL. Acta Metall Sin, 1980, 16(3): 331-377.

Download:  PDF(2054KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An investigation of the relationships between cold bending plasticity and micro-structures of welded joints in hot-rolled silicon steel coil in welded and heat-treatedconditions has been carried out by optical microscopy, TEM, SEM, and stressanalysis. It is shown that the martensite and carbide formed in weld junctionsand overheated zones as well as the coarse grains in the overheated zones are themain factors responsible for the welded joint fracture. The intersection of numerousdeforming twins in the overheated zones during deformation and their impactagainst phase boundaries also leads to an initiation of cracks. thus promoting thebrittle fracture of the welded joints.
Received:  18 March 1980     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1980/V16/I3/331

[1] Hull, D., Acta Met., 9 (1961) , 191.
[2] Gell, M. and Worthington, P. J., Acta Met., 14 (1966) , 1265.
[3] Worthington, P. J. and Smith, E., Acta Met., 14 (1966) , 35.
[4] Anderson, E. and Spreadborough, J., J. Iron Steel Inst., 206 (1968) , 1223.
[5] Leslie, W. C., Fischer, R. M. and Sen, N., Acta Met., 7 (1959) , 632.
[6] Leslie, W. C., Rickett, R. L., Stroble, C. P. and Konoval, G., Trans. ASM, 53 (1961) , 715.
[7] Konoval, G., Zwell, L., Dorman, L. A. and Leslie, W. C., Nature, 184 (1959) , 1863.
[8] McMahon, C. J. Jr. and Cohen, M., Acta Met., 13 (1965) , 591.
[9] Aronsson, B. and Granas, L., Met. Trans., 2 (1971) , 1087.
[10] McMahon, C. J. Jr., Acta Met., 14 (1966) , 839.