THE FORMATION OF Ni_5Hf AND THE SECONDARY CARBIDE IN HAFNIUM-BEARING CAST SUPERALLOYS
Zheng Yunrong;Cai Yulin
Cite this article: 

Zheng Yunrong;Cai Yulin. THE FORMATION OF Ni_5Hf AND THE SECONDARY CARBIDE IN HAFNIUM-BEARING CAST SUPERALLOYS. Acta Metall Sin, 1980, 16(2): 151-253.

Download:  PDF(3104KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The Ni_5Hf phase in hafnium-bearing nickle-base cast superalloys has beenexamined. It was found hat the reactions occurring in this series of alloys mightbe described as follows:Ni_5Hf+γ(C)-MC)_(2)+γor '(Hf)+γ(C)-MC_(2)+γThe effects of these reactions on the stability of the alloys have been discussed.
Received:  18 February 1980     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1980/V16/I2/151

[1] Kotval, P. S., Venables, J. D. and Calder, R. W., Met. Trans., 3 (1972) , 453.
[2] Dahl, J. M., Danesi, W. F. and Dunn, R. G., Met. Trans., 4 (1973) , 1087.
[3] Collins, H. E., Met. Trans., 5 (1974) , 189.
[4] Sims, C. T. and Hagel, W. C., The Superalloys, Wiley, New York, 1972, p. 275.
[5] Restall, J. E. and Toulson, E. C., Metals Mater., 7 (1973) , 187.
No related articles found!
No Suggested Reading articles found!