Abstract The microstructure changes in the tempering process of a quenched 6Cr4Mo3Ni2WV Matrix steel have been studied by TEM. Special attention has been paidto the observation of the microstuctures near the peak of the hardness-temperingtemperature curve. It is shown that, the secondary hardening of the steel is main-ly brought about by the precipitation of V_4C_3 and M_2C. With the tempering tempera-ture below 450℃ or so, the cementite lathes precipitated at the twin boundariesand {112} planes are fairly stable. However, they are transformed into a meta-stable phase, and finally are replaced by V_4C_3 M_2C and a new fine cementitewhen the tempering temperature is raised to beyond 500℃ This process certainlyleads to an increase in strength (secondary hardening), and what is more, it leadsto a substantial improvement in impact toughness in the meantime. The best impacttoughness is obtained by the time the cementite lathes are completely trans-formed. When tempering in the range of 600-650℃, the V_4C_3, M_ and alsothe fine cementite coalesced to equiaxed particles-M_6C or Cr_7C_3 at the austeniticgrain and sub-grain boundaries, and the impact toughness of the steel drops ac-cordingly.
|
Received: 18 January 1980
|
[1] 肖纪美,高速钢的金属学问题,冶金工业出版社,1976年. [2] Tekin. E. and Kelly, P.M., Precipitation from Iron-Base Alloys, Ed. by G.R. Speich and J.B. Clark, Gordon and Breach, New York, 1963,p. 173. [3] Marder, A.R., Benscoter, A.O. and Krauss, G., Met. Trans., 1 (1970) , 1545. [4] Kelly, P.M., and Nutting, J., J. Iron Steel Inst., 197 (1961) , 199. [5] 陈乾惕,金属学报,14(1978) ,432. [6] Hideji Suzuki, Sci. Rep. Res, Inst. Tohoku Univ.,Ser. A, 7 (1955) , 194. [7] Raynor, D., Whiteman, J.A. and Honeycombe, R. W. K., J. Iron Steel Inst., 204 (1966) , 349. [8] Kuo Kehsin (郭可信), J. Iron Steel Inst., 174 (1953) , 223. [9] Speich, G.R. and Leslie, W.C., Met. Trans., 3 (1972) , 1043. [10] Honeycombe, R.W.K., J. Iron Steel Inst., Spec. Rep., 1959, № 86, p. 1. [11] Raynor, D., Whiteman, J.A. and Honeycombe, R.W.K., J. Iron Steel Inst., 204 (1966) , 1114. [12] Nutting, J., J. Iron Steel Inst., 207 (1969) , 872. [13] 李春志,物理学报,28(1979) ,314. [14] #12 [15] Baker, G.R. and Nutting, J., J. Iron Steel Inst., Spec. Rep., 1959, № 64, p. 1. [16] Dyson, D.J., Keown, S.R., Raynor, D. and whiteman, J.A., Acta Met., 14 (1966) , 867.U |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|