THE EFFECT OF DECARBURIZING PROCESS ON THE MAGNETIC PROPERTIES OF THE GRAIN ORIENTED 3%Si-Fe |
Luo Yang;Zhang Baicheng;Zhou Xiuyuan;Ma Hongliang |
|
Cite this article:
Luo Yang;Zhang Baicheng;Zhou Xiuyuan;Ma Hongliang. THE EFFECT OF DECARBURIZING PROCESS ON THE MAGNETIC PROPERTIES OF THE GRAIN ORIENTED 3%Si-Fe. Acta Metall Sin, 1980, 16(1): 38-130.
|
Abstract The effect of decarburizing process on the magnetic properties of the grainoriented 3%Si-Fe has been studied. An empirical expression for the rate of decar-burization under given conditions was proposed. While the time of decarburizationwas given, the carbon content in 3%Si-Fe might be predicted, and vice versa.Another empirical expression for the rate of grain growth was also derived fromobservation of normal grain growth during decarburization. Based upon the aforementioned expressions, the functional dependence of thecarbon content before secondary recrystallization and time required for decarburi-zation on final magnetic properties of the grain oriented 3%Si-Fe has been dis-cussed. A two-demensional plot was then drawn on which the decarburizing pro-cess would be easily determined to acquire materials of superior quality.
|
Received: 18 January 1980
|
[1] 钢铁研究院硅钢研究组,金属学报,13(1977) ,80. [2] #12 [3] 中国科学院数学研究所统计组,常用数理统计方法,科学出版社,1973年. [4] Beck, P.A. Kremer, J.C., Demer, L.J. and Holzworth, M.L. Trans. AIME, 175 (1948) , 372. [5] Coble, R.C., J. Appl. Phys., 32 (1961) , 793. [6] Hu, H. and Rath, B. B. Met. Trans., 1 (1970) , 3181 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|