Abstract The effect of carbon and boron on the stress rupture properties at 600 and750℃ as well as on the tensile properties at room temperature and 650℃ of a35Ni15Cr type iron base alloy has been investigated. Both carbon and boronseemed to be markedly influential in the stress rupture life of the alloy whichreached its peak value with 0.03--0.05%C and about 0.006% B. However, thenotched-rupture sensitivity was hardly affected. The increment of boron content maycause lowering the eutectic temperature of boron-γ phase. The amount of borideeutectic increases with the increase of boron content and the solution treatmenttemperature. Minute boron-γ phase eutectic less affected the room temperaturetensile properties, but markedly shortened the rupture life.
|
Received: 18 January 1980
|
[1] 郭建亭,朱耀宵,师昌绪,金属学报,10(1974) ,74. [2] 铁基高温合金研究组,金属学报,14(1978) ,227. [3] 铁基高温合金研究组,金属学报,14(1978) ,348. |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|