| QUANTITATIVE PHASE ANALYSIS BY X-RAY WITHOUT ANY STANDARD IN TEXTURED MATERIALS |
| Lin Shuzhi Institute of Metal Research; Academia Sinica |
|
Cite this article:
Lin Shuzhi Institute of Metal Research; Academia Sinica. QUANTITATIVE PHASE ANALYSIS BY X-RAY WITHOUT ANY STANDARD IN TEXTURED MATERIALS. Acta Metall Sin, 1979, 15(2): 266-273.
|
|
|
Abstract Formulae derived for X-ray quantitative phase analysis without any standardin the case of specimens with identical texture have been shown to be in completeagreement with those derived by Zevin for randomly oriented specimens. Thus,when it is practicable by some ways (for example, by certain heat treatments) tochange the composition of the alloy phases without altering the texture of thespecimen, the method of quantitative phase analysis for such a textured specimencan be taken as identical with that for randomly oriented specimens. In cases where the absorption coefficients of the phases in a specimen happento be large, corrections for microabsorption are necessary and such corrections aregiven in the present work. The method mentioned above has been applied to a cold-rolled Fe-25%Mnalloy as well as to certain compacting specimens of Mo-Cu powders with satisfac-tory results.
|
|
Received: 18 February 1979
|
[1] Zevin, L. S., J. Appl. Crystallogr., 10 (1977) , 147. [2] Klug, H. P. and Alexander, L. E., X-Ray Diffraction Procedures for Polycrystalline and Amorphous Materials, 2nd ed., Wiley, New York, 1974, p. 532. [3] Chung, F. H., J. Appl. Crystallogr., 7 (1974) . 519. [4] Biederman, R. R. et at., Advances in X-Ray Analysis, Vol. 17, Plenum, New York, 1974, p. 139. [5] 1974. [6] Lopata, S. L. and Kula, E. B., Trans. AIME, 233 (1965) , 288. [7] Van Niekerk, M. N. and Argent, B. B., J. Iron Steel Inst., London, 208 (1970) , 779. [8] 木村希夫, 日本金属学会志,36(1972) ,545. [9] Brindley, G. W., Phil. Mag., 36 (1945) , 374. [10] X射线结构分析,龚尧圭等译,科学出版社,1958年,p.237. [11] 沈鹏,金属学报,12(1976) ,111. |
| No Suggested Reading articles found! |
|
|