					Cite this article:
						|  |  
    					|  |  
    					| AN INVESTIGATION OF QUASI-CLEAVAGE FRACTURE IN STEEL |  
						| Liao Chienchu;Sun Fuyu;Lan Fenlan Beijing Institute of Iron and Steel Research |  
						|  |  
					
			      Liao Chienchu;Sun Fuyu;Lan Fenlan Beijing Institute of Iron and Steel Research. AN INVESTIGATION OF QUASI-CLEAVAGE FRACTURE IN STEEL. Acta Metall Sin, 1979, 15(2): 259-313.	
				 
					
						| 
								
									|  
          
          
            
              
				
												  
													
													    |  |  
														| Abstract  The quasi-cleavage fracture has been studied in conjunction with the stressstrain behaviour of steel specimens. Consideration of the results obtained on dif-ferent varieties of steel indicate that the quasi-cleavage fracture may be interpretedin terms of certain transition fracture mechanism as follows: Microcleavage cracks are nucleated at certain places of high tensile strss con-centration, subsequently each of them propagates along the cleavage plane in grainsalready deformed and finally they merge together by microplastic coalescence.According to the above conception, the interaction between the cleavage crack andthe plastic deformation may be regarded as the most important characteristics ofquasi-cleavage fractures. Using quantitative fractography, correlation between thefractographic features of specimens and the parameters of its certain mechanicalproperties may be established. |  
															| Received:  18 February 1979 |  
            
									            
									               
																												  
															| [1] Beachem, C. D. and Relloux, R. N., Amer. Soc. Test. Mater., Spec. Tech. Publ. № 381, ASTM, 1964, p. 210. [2] Sullivan, C. P., Weld. Res. Counc. Bull., (1967) , May, 122.
 [3] Thomas, K. S., Klingcle, H. and Woitscheck, A., Pract. Metallogr., 11 (1970) , № 10, 538.
 [4] Matsuda, S., Trans. Jap. Inst. Metals, 11 (1970) , 371.
 [5] Terasaki, T., Trans. Iron Steel Inst. Jap., 12 (1972) , 45.
 [6] Beachem, C. D., Met. Trans., 4 (1973) , 1999.
 [7] Evans, P. K. V.. J. Iron Steel Inst., London, 210 (1972) . 200.
 [8] 北京钢铁研究院,工程断裂力学,上册,国防工业出版社,1977年,p.106.
 [9] 饭田国广,金属材料,12(1972) ,№ 3,85.
 [10] 北京钢铁研究院,长时运行的12CrlMoV主蒸汽管试验总结,1977年.
 [11] 廖乾初, 未发表工作.
 [12] 陈箎,私人通讯.
 |  
             
								                
															
																| 
																																																																									