Abstract An investigation of the structures of Ni-Fe-Mo and Ni-Fe-Nb alloys has beencarried out by means of TEM supplemented by electron diffraction and X-ray dif-fraction analysis. The results obtained have been correlated with magnetic proper-ties as follows: Both alloys showed modulated structures, in which the Ni-Fe-Nb alloy beingcoarser and more predominant. As the proportion of modulated structures increases,the hardness of the alloy also increases, but vice versa in the case of its mag-netic permeability. The introduction of solute atoms Mo and Nb would lower the degree of or-dering in Ni_3Fe alloy, but fortunately only certain degree of ordering was sufficientto yield conditions for high permeability. A preprecipitating phase possessing thefcc (ordered) Ni_3Nb (γ′) structure and being coherent with the matrix,was observ-ed in the Ni-Fe-Nb alloy. This phase appears to promote the formation of modu-lated structures and exert a strengthening effect on matrix.
|
|
Received: 18 February 1979
|
[1] Berkowitz, A. and Kweller, E., Magnetism and Metallurgy, Vol. 2, Academic, New York, 1969, p. 550. [2] Bozorth, R. M., Ferromagnetism, D. Van Nostrand Co., Toronto, 1953, p. 134. [3] 增本量,日本金属学会志,35(1971) ,985. [4] 比内正胜,日本金属学会志,40(1976) ,682. [5] Bourgeot, J., Mem. Sci. Rev. Met., 66 (1969) , 845. [6] 戴礼智,王俊健,侯德惠,金属学报,12(1976) ,102. [7] 郭可信,X射线学及电子显微术的进展,上海科技出版社,1966年,p.36. [8] 宫崎亨,日本金属学会会报,15(1976) ,309. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|