| ON THE RELATION BETWEEN INCLUSIONS AND MORPHOLOGY OF DIMPLE FRACTURES IN CERTAIN STEELS |
| Zhao Jian |
|
Cite this article:
Zhao Jian. ON THE RELATION BETWEEN INCLUSIONS AND MORPHOLOGY OF DIMPLE FRACTURES IN CERTAIN STEELS. Acta Metall Sin, 1978, 14(3): 316-348.