| TREATMENT OF EXTINCTION PROBLEMS IN THE AUTOMATIC CALCULATION OF FUNDAMENTAL DATA OF RECIPROCAL LATTICE PLANES |
| Wang Ren-hui Kang Li-shan(Wuhan University) Sun Tian-xi Wan Xian(Research Institute of Wuhan Iron and Steel Company) |
|
Cite this article:
Wang Ren-hui Kang Li-shan(Wuhan University) Sun Tian-xi Wan Xian(Research Institute of Wuhan Iron and Steel Company). TREATMENT OF EXTINCTION PROBLEMS IN THE AUTOMATIC CALCULATION OF FUNDAMENTAL DATA OF RECIPROCAL LATTICE PLANES. Acta Metall Sin, 1978, 14(3): 304-309.
|
|
|
Abstract A computer program has been given for calculating the fundamental data of reciprocal lattice planes, with special attention paid to the problem of systematic extinctions for phase analysis by electron diffraction methods. Satisfactory results have been obtained in the cases of diamond, spinel as well as hexagonal closepacked structures.
|
|
Received: 18 March 1978
|
[1] 金属研究所电镜实验室,金属学报,11,(1975) ,183. [2] Booth, M. et al., Met. Trans., 5 (1974) , 775. [3] Bucksch, R., J. Appl. Cryst., 6 (1973) , 304. [4] Meakin, J. D., Trans. AIME, 245 (1969) , 170. [5] Maucione, C. M. et al., Met. Trans., 2 (1971) , 2289. [6] 金属研究所电镜实验室,金属学报,12(1976) ,198. [7] 成田贵一,松本洋,鉄鋼,58(1972) ,1330. [8] Structure Reports for 1954, vol. 18, p. 262 |