| AN INVESTIGATION OF THE CRACK-TIP STRESS AND STRAIN |
| Deng Zhi-sheng Chen Chi (Chen Chih)(Beijing Institute of Iron and Steel Research) |
|
Cite this article:
Deng Zhi-sheng Chen Chi (Chen Chih)(Beijing Institute of Iron and Steel Research). AN INVESTIGATION OF THE CRACK-TIP STRESS AND STRAIN. Acta Metall Sin, 1978, 14(3): 239-326.
|
|
|
Abstract With the aid of etching by Fry's reagent and microhardness measurements, the crack-tip stress and strain have been investigated. The results obtained may be summarized as follows:The crack-tip stress increases simultaneously with the angle of bend of the specimen in accord with the relationJ=G+[(β/3~(1/2)+1/2(σ_(YY))_A)]δ_p derived by us under the linear hardening law:■=β+γ■until the critical point is reached:J_c=G_c+(β/3~(1/2)+1/2σ_F)δ_(p,c) demonstrating that at the critical point(σ_(YY))_A=σ_F
|
|
Received: 18 March 1978
|
[1] 陈篪,金属学报,13(1977) .57;Scientia Sinica,ⅩⅪ(1978) ,112. [2] 陈篪,待发表工作. [3] 希尔,R,塑性数学理论,王仁等译,科学出版社,1966年,282页. [4] 陈篪,待发表工作. [5] 陈篪等,金属学报,11(1975) ,174.Y |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|