AN OBSERVATION OF UNHEALED POROSITIES AND CRYSTALLINE STEPS IN ALUMINIUM ALLOY FORGINGS
Zhou Jing Chang Xin Guo Ke-xin (Kuo Ke-hsin)(Institute of Metal Research; Academia Sinica)
Cite this article: 

Zhou Jing Chang Xin Guo Ke-xin (Kuo Ke-hsin)(Institute of Metal Research; Academia Sinica). AN OBSERVATION OF UNHEALED POROSITIES AND CRYSTALLINE STEPS IN ALUMINIUM ALLOY FORGINGS. Acta Metall Sin, 1978, 14(3): 246-329.

Download:  PDF(4127KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Unhealed porosities and free surface of dendrites with crystalline steps were occasionally observed in aluminium alloy forgings. It was found that the dendrites grow preferentially along <100> directions and the crystalline steps belong mainly to {100} and {110} planes.In the neighbourhood of the unhealed porosities the alloy matrix appeared to be embrittled and in certain cases cleavage fracture was observed.
Received:  18 March 1978     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1978/V14/I3/246

[1] Ryder, D. A., Acta Met., 9 (1961) , 73.
[2] Mencarelli, E. et al., Mere. Sci. Rev. Met., 63 (1966) , 407.
[3] Gruhl, W., Aluminium, 38 (1962) , 775.
[4] Fractography and Atlas of Fractographs, 8th ed., ASM Metals Handbook, Vol. 9, Amer. Soc. Metals, Ohio, (1974) .
[5] #12
[6] Kocanda, S. and Kozubowski, J., Arch. Hutn., 16 (1971) , 221.
[7] Kocanda, S. and Kozubowski, J., Z. Metallk., 65 (1974) , 453.
[8] Graf, L., Z. Metallk., 42 (1951) , 336.
[9] Walton, D. and Chalmers, B., Trans. AIME, 215 (1959) , 447.
[10] Hayashi, T. et al., Jap. J. AppI. Phys., 16 (1977) , 705.
[11] Kimoto, K, et al., ibid, 16 (1977) , 941.
[12] Nelson, R. S. et al., Phil. Mag., 11 (1955) , 91.
[13] Sundqvist, B. E., Acta Met., 12 (1964) , 67.
[14] Foss, D. and Herbj(?)rnsen, O. H., Phil. Mag., 13 (1966) , 945.
[15] Hess, P. D. and Turnbull, G. K., Hydrogen in Metals, Number 2 in the Materials/Metalworking Technology Series, ed. by I. M. Bernstein and A. W. Thompson, (1974) , 277.
[16] 陈廉等,金属学报,14(1978) ,253
No related articles found!
No Suggested Reading articles found!