| AN INVESTIGATION OF INTERNAL CRACKS IN THE CONTINUOUS CASTING BILLETS AND ROLLING PRODUCTS OF A 0.45% C STEEL |
| Joint Res. Gp.; Institute of Metal Research and Dalian Steel Works |
|
Cite this article:
Joint Res. Gp.; Institute of Metal Research and Dalian Steel Works. AN INVESTIGATION OF INTERNAL CRACKS IN THE CONTINUOUS CASTING BILLETS AND ROLLING PRODUCTS OF A 0.45% C STEEL. Acta Metall Sin, 1978, 14(2): 165-241.
|
|
|
Abstract In certain conditions, hot cracks eccurred in continuous casting billets of a 0.45% C steel. It was observed that such cracks were practically healed by rolling when the reduction ratio attained about four. Inclusion clusters and segregation of phosphorous in the neighbourhood of the above cracks as elongated streaks were often present and aligned with the rolling direction. In view of these, dark etching lines resembling cracks could occur on deep macro-etching. This sort of inhomogeneity hardly affected the longitudinal mechanical properties of therolling products, although the transverse ductility was appreciably lowered.
|
|
Received: 18 February 1978
|
[1] Drunen, G. Van et al., Ironmaking Steelmaking, 2 (1975) , 125. [2] Baker, T. J. and Charles, J. A., J. Iron Steel Inst., 210 (1972) , 702. [3] Lankford, W. J., Met. Trans., 3 (1972) , 1331. [4] Adams, C. J., Open Hearth Proc., 54 (1971) , 290. [5] Miller, C. I., ibid, 54 (1971) , 316. [6] Baumann, H. G. et al., Baender, Bleche, Rotate, 12 (1971) , № 6, 239. [7] Mills, N. T. and Joseph, R. W., Ironmaking Steelmaking, 4 (1977) , 181. [8] “晶间裂纹”三结合研究组,金属学报,10(1974) ,p.41. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|