    					| AN INVESTIGATION OF CERTAIN INTERGRANULAR CRACKS IN THE CORE OF A 20Cr2Ni4A STEEL BILLET |  
						| Tian Ji-feng Liu Xing-zhi and Wei Kun |  
						|  |  
					
			      Tian Ji-feng Liu Xing-zhi and Wei Kun. AN INVESTIGATION OF CERTAIN INTERGRANULAR CRACKS IN THE CORE OF A 20Cr2Ni4A STEEL BILLET. Acta Metall Sin, 1978, 14(2): 171-252.	
				 
					
						| 
								
									|  
          
          
            
              
				
												  
													
													    |  |  
														| Abstract  An investigation has been carried out on the so-called intergranular cracks appearing in the central part of a macroetched transverse section of a 20Cr2Ni4A steel billet. It is shown that this in fact was a kind of acid-etching phenomenon, due to low-melting inclusions at the interdendritic boundaries appearing as cracks. The above observation was further substantiated in laboratory ingots by the introduction of certain low-melting inclusions into experimental melts. |  
															| Received:  18 February 1978 |  
            
									            
									               
																												  
															| [1] “晶间裂纹”三结合研究小组,金属学报,10(1974) ,41. [2] 金属研究昕,大连钢厂联合研究组,金属学报,14(1978) .
 [3] Sims, C. E., Trans. AIME, 215 (1959) , 367.
 |  
             
								                
															
																| 
																																																																									
																				| No Suggested Reading articles found! |  |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |