Abstract  The stress intensity factors of a single-edge cracked bar loaded by in-planetransverse forces are calculated with the application of the principle of superposition, and St. Venant's Principle. Simple formulae for K_Ⅰ and K_Ⅱ are derivedand the appropriate conditions under which these formulae are applicable havebeen discussed.
Received:  18 April 1977     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1977/V13/I4/301

[1] 陈篪,力学,(1974) ,№ 3,121.
[2] Brown, W. F. Jr. and Srawley, J. E., Amer. Soc. Test. Mater., Spec. Tech. Publ., No. 410, (1966) .
[3] Srawley, J. E. and Gross, B., Eng. Fract. Mech., 4 (1972) , 587.
[4] Wilson, W. K., Eng. Fract. Mech., 2 (1970) , 169.
[5] Benthem, J. P. and Koiter, W. J., Mechanics of Fracture, vol. Ⅰ, ed. by G. C. Sih, Noordhoff International Publishing, Leyden, the Netherlands, (1973) , 131.
[6] Tada, H., Paris, P. C. and Irwin, G. R., The Stress Analysis of Crack Handbook, Del Research Corp., Hellertown, Pa., U. S. A., 1973.-
No related articles found!
No Suggested Reading articles found!