Please wait a minute...
Acta Metall Sin  1977, Vol. 13 Issue (4): 289-365    DOI:
Current Issue | Archive | Adv Search |
AN INVESTICATION OF A MARAGING STEEL WITH LOWER Ni AND Co CONTENTS
Tsai Chi-kung;Chu Ching;Ho Chung-chih;Shen Hui-wang;Luo Li-keng;Sung Wei-shun;Yu Wei-le Peking Institute of Iron and Steel Research
Cite this article: 

Tsai Chi-kung;Chu Ching;Ho Chung-chih;Shen Hui-wang;Luo Li-keng;Sung Wei-shun;Yu Wei-le Peking Institute of Iron and Steel Research. AN INVESTICATION OF A MARAGING STEEL WITH LOWER Ni AND Co CONTENTS. Acta Metall Sin, 1977, 13(4): 289-365.

Download:  PDF(3584KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  It is shown that Cr and Mn bearing 12Ni maraging steels with lower Niand Co contents are of high strength and toughness, Precipitates after aging,dislocation configurations and easy cross-slip behavior of dislocations have beenexamined. The results are discussed on the assumption that the hexagonal close-packed phases were precipitated along the stacking fault zone of the dislocationlines. In order to predict the stability and solubility of high-temperature austenitein maraging steels, a criterion has been suggested from the point of view ofaverage electron concentration per atom of the alloy. The criterion is helpful forrational alloying of maraging steels with lower Ni and Co contents.
Received:  18 April 1977     

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1977/V13/I4/289

[1] 蔡其巩、朱静、何崇智,物理学报,23(1974) ,178.
[2] Steinen, A. and Schuben, F., DEW-Tech. Ber., 9 (1969) .
[3] Srawlay, J. E. and Brown, W. F., Plane Strain Crack Toughness Testing of High Strength Metallic Materials, Amer. Soc. Test. Mater., Spec. Tech. Publ., No. 410, (1966) , pp. 1--65.
[4] Patterson, R. L. and Wayman, C. M., Acta Met., 14 (1966) , 347.
[5] Banerjee, B. R. et al., Metal Sci. J., 2 (1968) , 77.
[6] Detert, K., Trans. AIME, 239 (1967) , 553.
[7] Squires, D. R. and Wilson, E. A., Met. Trans., 3 (1972) , 575.8