[1] Brown, W. F. and Scrawloy, J. E., Amer. Soc. Test. Mater., Spec. Tech. Publ. No. 410 (1969) , 12. [2] Gerberich, W. W. and Katz, Y., Eng. Fract. Mech., 1 (1969) , 569. [3] Orange, T. W., Amer. Soc. Test. Mater., Spec. Tech. Publ. No. 513 (1972) , 75.} |