| SOME PROBLEMS CONCERNING THE J_Ic DETERMINATION BY MEANS OF A SINGLE SPECIMEN |
| Res. Gp. of Fracture Toughness; Peking Institute of Iron and Steel Research |
|
Cite this article:
Res. Gp. of Fracture Toughness; Peking Institute of Iron and Steel Research. SOME PROBLEMS CONCERNING THE J_Ic DETERMINATION BY MEANS OF A SINGLE SPECIMEN. Acta Metall Sin, 1977, 13(3): 214-258.
|
|
|
Abstract The present paper deals with the method of locating the crack initiation point inJ_(IC) determinahon by means of a single specimen. The first is an analytical method forcalculating crack length variations during monotonic loading from the load-displace-ment record alone, and the second is based on And-sectional measurements of C. T. O. D.Results of application of these methods are presented which demonstrate the effective-ness of the methods proposed. In additional, some recent experimental results are also reported which substanti-ate the slip-line field proposed earlier for the CT specimen, the result for the limit loadP_L, and the J-U relation obtained by us.
|
|
Received: 18 March 1977
|
[1] 陈篪、姚蘅、邓枝生、庄韬、邓其源,科学通报,(1975) ,329. [2] 陈篪,金属学报,12(1976) ,129. [3] 陈篪、姚蘅、邓枝生、庄韬、邓其源,金属学报,11(1975) ,174. [4] 陈篪,未发表工作. [5] Rice, J. R. et al., Amer. Soc. Test. Mater., Spec. Tech. Publ. No. 536, 1973, p. 231. [6] 陈篪、姚蘅、金志英,科学通报,(1974) , 41. [7] Roberts, E. Jr., Mater. Res. Stand., 9 (1969) , 27. [8] Ewing, D. J. F. and Richards, C. E., J. Mech. Phys. Solids, 22 (1974) , 27. [9] Feddern, G. and Macherauch, E., Proc. 3rd Int. Congr. Fracture, pt. Ⅲ. [10] Gross, B. et al., Int. J. Fract. Mech., 4 (1968) , 267. [11] Otsuka, A et al., Eng. Fract. Mech., 7 (1975) , 419. [12] Arii, M. et al., Eng Fract. Mech., 7 (1975) , 551. [13] Green, G. and Knott, J. F., J. Mech. Phys. Solids, 23 (1975) , 167. [14] Robinson, J. N. and Tetelman, A. S., Proc. 3rd Int. Congr. Fracture, pt. Ⅱ. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|