THE CHLORINATION EQUILIBRIUM OF CUPRIC OXIDE
HUANG CHIEN-K'ANG; PAO CH'AO; WEI CHAO-HSIUNG; CHU HAO-HSI; CHIN YEN-FU; CH'N HSIN-MIN
Cite this article: 

HUANG CHIEN-K'ANG; PAO CH'AO; WEI CHAO-HSIUNG; CHU HAO-HSI; CHIN YEN-FU; CH'N HSIN-MIN. THE CHLORINATION EQUILIBRIUM OF CUPRIC OXIDE. Acta Metall Sin, 1966, 9(1): 18-24.

Download:  PDF(497KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The chlorination equilibrium of cupric oxide has been investigated using the circulation method. Within the temperature range 300—450℃, the reaction is found to take place in two stages, and the following results are obtained:2CuO(s)+Cl_2(g)=Cu_2OCl_2(s)+1/2O_2(g), (1)logK_p~Ⅰ=(3061/T)-2.228,ΔG_Ⅰ~O=-14010+10.20T.Cu_2OCl_2(s)+Cl_2(g)=2CuCl_2(s)+1/2O_2(g), (2)logK_p~Ⅱ=(2370/T)-1.90,ΔG_Ⅱ~O=-10850+8.69T.The physical properties of the intermediate compounds have been studied, and within the given temperature range, the average enthalpy of formation of the intermediate compound Cu_2OCl_2 is found to be -84900 cal./mole; and its average entropy of formation to be -51.23 e.u.
Received:  18 January 1966     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1966/V9/I1/18

[1] Jellinek, K., Rudat, A.: Z. Anorg. Allgem. Chem., 1926, 155, 73.
[2] #12
[3] 陈新民、黄健康、鲍超等:金属学报,1965,9,4.
[4] Kubaschewski, O., Evans, LL.: Metallurgical Thermichemistry, 3rd ed., (Pergamon, 1958) , p. 236, 240, 242, 264, 314, 315, 320.%
No related articles found!
No Suggested Reading articles found!