THE CHLORINATION EQUILIBRIUM OF NICKELOUS OXIDE
PAO CH'AO; HUANG CHIEN-K'ANG; WEI CHAO-HSIUNG; CH'IEN HSIN-MIN
Cite this article: 

PAO CH'AO; HUANG CHIEN-K'ANG; WEI CHAO-HSIUNG; CH'IEN HSIN-MIN. THE CHLORINATION EQUILIBRIUM OF NICKELOUS OXIDE. Acta Metall Sin, 1966, 9(1): 13-17.

Download:  PDF(375KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The chlorination equilibrium of nickelous oxide has been investigated using the circulation method within the temperature range 666—928°K from both sides. The reaction is established as NiO(s)+Cl_2(g)=NiCl_2(s)+1/2O_2(g). The equilibrium constant and standard free energy of this reaction may be represented aslog K_p=(2720/T)-2.312ΔG_T~O=-12450+10.58 T.The result is found to be in good agreement with thermodynamic data in the literature. The maximum error for ΔG_T~O is estimated to be about +300 cal. At lower temperature, the experimental results of show some deviation from our data, probably due to unattainment of equilibrium in his experiments.
Received:  18 January 1966     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1966/V9/I1/13

[1] Jellinek, K., Rudat, A.: Z. Anorg. Allgem. Chem., 1926, 155, 73.
[2] #12
[3] 陈新民、黄健康、鲍超等:金属学报,1965,9,4.
[4] #12
[5] #12
[6] Kubaschewski, O., Evans, E. LL.: Metallurgical Thermochemistry, 3rd ed., (Pergamon, 1958) , p. 262, 320.
[7] #12
[8] #12
[9] #12=
No related articles found!
No Suggested Reading articles found!