THE TEMPERATURE COEFFICIENT OF SURFACE TENSION OF PURE COPPER
YEN SHUO Institute of Metal Research; Academia Sinica
Cite this article: 

YEN SHUO Institute of Metal Research; Academia Sinica. THE TEMPERATURE COEFFICIENT OF SURFACE TENSION OF PURE COPPER. Acta Metall Sin, 1965, 8(2): 251-258.

Download:  PDF(763KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The change of surface tension of molten copper with temperature was measured bymeans of the sessile drop method both on heating and on cooling. It is shown that thetemperature coefficient of surface tension is negative, being -0.470 dyne/cm·℃ at1100-1500℃. A maximum was observed on the surface tension-temperature curve at1350℃, indicating an apparent positive coefficient up to this temperature. This is ex-plained by the presence of residual surface active impurities in the original sample whichlowered the surface tension, and the removal of such impurities during heating.
Received:  18 February 1965     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1965/V8/I2/251

[1] Turnbull, D.: J. Chem. Phys., 1950, 18, 769.
[2] Залетаева, Р. П., Крещановский, Н. С., Кунин, Л. Л.: 1951, (2) , 26.
[3] Bailey, G. L. J., Watkins, H. C.: j. Inst. Metals, 1951, 80, 57.
[4] Humenik, Jr. M., Parikh, N. M.: J. Am. Ceram. Soc., 1956, 39, 60.
[5] Kingery, W. D.: Am. Ceram. Soc. Bull., 1956, 35, 108.
[6] Уманский,Я.С,Финкельштейн,Б.Н.,Влантер,М.Е.著,中国科学院金属研究所译:金属学物理基础,(科学出版社,1958年),200页.
[7] Самарин,А.М.著,邹元爔等译:钢脱氧的物理化学基础,(科学出版社,1958年),139页.
[8] 陈念贻、张桂成:科学通报,1963,(3) ,68.
[9] #12
[10] Quincke, G.: Ann. Phys., 1869, 138, 141.
[11] Herzfeld, R.: Ann. Phys., 1897, 62, 450.
[12] Holman, E. J. L.: J. Iron Steel Inst. (London), 1923, 107, 517.
[13] Libman, E. E.: Phys. Rev., 1927, 29, 911.
[14] Smith, S. W.: J. Inst. Metals 1914, 12, 168.
[15] #12
[16] Drath, G., Sauerwald, F.: Z. Anorg. Allgem. Chem., 1927, 162, 301.
[17] Krause, W., Sauerwald, F.: Z. Anorg. Allgem. Chem., 1929, 181, 353.
[18] #12
[19] #12
[20] #12
[21] Becker, G., Harders, F., Kornfeld, H.: Arch. Eisenhuttenw., 1949, 363.
[22] Baes, C. F., Kellogg, H. H.: Trans. AIME, 1953, 197, 643.
[23] Kozakevitch, P., Chatel, S. Urbain, G. et al.: Rev. Met., 1955, 52, 139.
[24] Allen, B. C., Kingery, W. D.: Trans. AIME, 1959, 215, 30.
[25] #12
[26] 门间改三、须藤一:日本金属学会志,1960, 24, 374.
[27] Whalen, T. J., Humenik, M. Jr.: Trans. AIME, 1960, 218, 952.
[28] #12
[29] Metzger, G.: Z. Phys. Chem., 1959, 211, 1.
[30] Pawlek, F., Thielsch, W., Wuth, W.: Metall, 1961, 15, 1076.
[31] Gans, W., Pawlek, F., von Ropenack, A.: Z. Metallk., 1963, 54, 147.
[32] Bashforth, F., Adams, S. C.: An Attempt to test the theories of capillary action (Cambridge, 1883) .
[33] Urbain, G., Lucas, L. D.: The Physical Chemistry of Metallic Solutions and Intermetallic Compounds, National Physical Laboratory Symposium, (H. M. Stationery Office, 1959) , vol. 2, No. 9, 4E.
[34] Hartmann, R., Schneider, R.: Z. Anorg. Allgem. Chem., 1929, 180. 275.
[35] #12
[36] White, D. W. G.: Trans. Am. Soc. Metals, 1962, 55, 757.
[37] Kozakevitch, P.: The Physical Chemistry of Metallic Solutions and Intermetallic Compounds, National Physical Laboratory Symposium (H. M. Stationery Office, 1959) , vol. 1, No. 9, 1E.
[38] Kurkjian, C. R., Kingery, W. D.: J. Phys. Chem., 1956, 60, 961.
[39] Kingery, W. D., Humenik, M. Jr.: J. Phys. Chem., 1953, 57, 359.
[40] Cahill, J. A., Kirshenbaum, A. D.: J. Phys. Chem., 1962, 66. 1080.
No related articles found!
No Suggested Reading articles found!