DISTRIBUTION OF LEAD, TIN AND MAGNESIUM BETWEEN LIQUID GALLIUM AND MERCURY
LI AI-CHEN;CHOU YUAN-HSI Institute of Metallurgy; Academia Sinica
Cite this article: 

LI AI-CHEN;CHOU YUAN-HSI Institute of Metallurgy; Academia Sinica. DISTRIBUTION OF LEAD, TIN AND MAGNESIUM BETWEEN LIQUID GALLIUM AND MERCURY. Acta Metall Sin, 1965, 8(2): 193-196.

Download:  PDF(279KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The distribution of lead and tin between liquid gallium and mercury has been studiedover a suitable concentration range at three temperatures. The distribution coefficientsobtained from the experimental data are plotted against the composition of the galliumphase, and the shape of the curves is briefly discussed. Besides, the distribution coefficient for magnesium between liquid gallium and mer-cury has been determined for a single concentration at 35℃.
Received:  18 February 1965     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1965/V8/I2/193

[1] 刘民治:物理学报,1959,15,389。
[2] Pierre De La Breteque: Preparation of Ⅲ--Ⅴ Compounds, (Reinhold, 1962) , p. 68.
[3] Plust, H. G.: Ger. (West) Patent, No. 1,002,012, 1956.
[4] Spicer, W. M., Bartholomay, H. W.: J. Am. Chem. Soc., 1951, 73, 868.
[5] #12
[6] Rand, M. H., Kubaschewski, O.: The Thermochemical Properties of Uranium Compounds, (Oliver & Boyd, 1963) , p. 52.
[7] Kubaschewski, O., Catterall, J. A.: Thermochemical data of Alloys, (Pergamon, 1956) , p. 101, 104.
No related articles found!
No Suggested Reading articles found!