Abstract  Vacuum melted and cast electrolytic iron bar, 10 mm in diameter, has been refinedby the floating-zone technique for eleven passes in an atmosphere of hydrogen. Thetravel rate of the zone was 1-2 mm/min and the lower chuck was rotated at a speed of3.5-22 rpm. On the basis of the measured distribution coefficient of carbon and metallographicexamination of the non-metallic inclusions the possibility of removing carbon and oxygenfrom iron by floating-zone melting is discussed.
Received:  18 February 1965     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1965/V8/I2/197

[1] Keck, P. H., Golay, M. J. E.: Phys. Rev., 1953, 89, 1297.
[2] Cunnell, F. A., Wickham, R.: J. Sci. Instr., 1960, 37, 410.
[3] Bardsley, W.: Res. Appl. Ind., 1959, 12, 183.
[4] Oliver, B. F., Shafer. A. J. Trans. AIME. 1960. 218. 194.
[5] 京谷益次、绕木路南、西川和幸:日本金属学会志,1960,24,391.
[6] Smith, R. L., Rutherford, J. L.: Trans. AIME, 1957, 209, 478.
[7] Fischer, W. A., Spitzer, H., Hishinuma, M.: Arch. Eisenhuttenw., 1960, 365.
[8] Hillmann, H., Mager, A.: Z. Metallk., 1960, 51. 663.
[9] 中村卫:日本金属学会志,1962,26,391。
[10] Williams, W. M., Craig, G. B., Winegard, W. C.: Can. Mining Met. Bull., 1962, 55, 35.
[11] Simonsen, E. B.: J. Iron Steel Inst. (London). 1962, 200, 193.
[12] 大岡耕之、三村宏、矢野清之助等:日本金属学会志,1963,27,342.
[13] 何焕南、严荣华、俞柏华:改良低压燃烧法测定金属中微量碳,待发表.
[14] Chipman, J.: Basic Open Hearth Steelmaking, 2nd ed., (AIME, 1951) , p. 632.
[15] Hayes, A., Chipman, J.: Trans. AIME 1939, 135, 85.
[16] Hansen, M.: Constitution of Binary Alloys, 2nd ed., (McGraw-Hill, 1958) .
[17] Tiller, W. A.: J. Iron Steel Inst. (London), 1959, 192, 338.
[18] #12
[19] Pfann, W. G.: Zone Melting, (Wiley, 1958) , p. 16.
[20] Darken, L. S.: Basic Open Hearth Steelmaking, 2nd ed., (AIME, 1951) , p. 610.
[21] Seybolt, A. U.: J. Metals, 1954, 6, 979.
[22] Pfann, W. G.: Science, 1962, 135, 1101.
[23] Wroughton, D. M., Okress, E. C., Brace, P. H. et al.: J. Electrochem. Soc., 1952, 99, 205.
No related articles found!
No Suggested Reading articles found!