ДИАГРАММЫ СОСТОЯНИЯ СИСТЕМ KCl-TiCl_2 И NaCl-TiCl_2
Ли Си-чан
Cite this article: 

Ли Си-чан. ДИАГРАММЫ СОСТОЯНИЯ СИСТЕМ KCl-TiCl_2 И NaCl-TiCl_2. Acta Metall Sin, 1965, 8(2): 187-192.

Download:  PDF(417KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  ~~
Received:  18 February 1965     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1965/V8/I2/187

[1] Ehrlich, P., Kuhnl, H.: Z. Anorg. Allgem. Chem., 1957, 292, 146.
[2] Komarek, K., Herasymenko, P.: J. Electrochem. Soc., 1958, 105, 210.
[3] Komarek, K., Herasymenko, P.: J. Electrochem. Soc., 1958, 105, 216.
[4] Ehrlich, P., Schmitt, R.: Z. Anorg. Allgem. Chem., 1961, 308, 91.
[5] #12
[6] 黎锡强:金属学报,1965,8,24。
[7] #12
[8] #12
[9] #12
[10] #12
[11] #12
No related articles found!
No Suggested Reading articles found!