| THE TEXTURE AND MAGNETOSTRICTION OF NICKEL |
| CHANG HSIN-YU;CHEN YU-LIEN;TAI LI-CHI |
|
Cite this article:
CHANG HSIN-YU;CHEN YU-LIEN;TAI LI-CHI. THE TEXTURE AND MAGNETOSTRICTION OF NICKEL. Acta Metall Sin, 1965, 8(1): 93-97.
|
|
|
Abstract An investigation on the rolling and recrystallization textures of nickel has beencarried out. After different reductions, the transformation of the rolling texture and themagnetostriction of the cube-textured material are studied. The change of length of thecube-textured specimens in a magnetic field is similar to that of a single crystal in [100]direction; as the percentage of reduction increases, the magnetostriction is more difficultto reach saturation.
|
|
Received: 18 January 1965
|
[1] Masiyama, Y.: Sci. Rept. Res. Inst. Tohoku Univ., 1928, 17, 945. [2] Smallman, R. E.: J. Inst. Metals, 1955--56, 84, 10. [3] Clark, C. A., Mee, P. B.: Z. Metallk., 1962, 53, 64. [4] #12 [5] 戴礼智、张信钰、刘壬宝:金属学报,1959,4,51. [6] Paces, J., Suda, P.: Czech. J. Phys., 1961, 11, 439. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|