THE MAGNETIC ANNEALING AND INDUCED ANISOTROPY IN FERROMAGNETIC ALLOYS
TAI LI-CHI
Cite this article: 

TAI LI-CHI. THE MAGNETIC ANNEALING AND INDUCED ANISOTROPY IN FERROMAGNETIC ALLOYS. Acta Metall Sin, 1965, 8(1): 108-136.

Download:  PDF(2532KB) 
Export:  BibTeX | EndNote (RIS)      
Received:  18 January 1965     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1965/V8/I1/108

1) G. W. Elmen: Bell System Tech. J., 1936, 15, 113.
2) 见Sci. Rept. Res. Inst. Tohoku Univ., 1958, A 10, 34.
1) Sucksmith, W., Thompson, J. E.: Proc. Roy. Soc. 1954, A225, 362.
1) 参阅 Aoyagi, K.: Sci. Rept. Res. Inst. Tohoku Univ., 1961, A13, 137.
[1] Kelsall, G. A.: Physics, 1934, 5, 169.
[2] Dillinger, J. F., Bozorth, R. M.: Physics, 1935, 6, 279.
[3] Bozorth, R. M., Dillinger, J. F.: Physics, 1935, 6, 285.
[4] Bozorth, R. M.: Ferromagnetism, (Van Nostrand, 1951) , p. 119.
[5] Becker, J. J.: Met. Rev., 1962, 7, 371.
[6] Gould, H. L. B., Wenny, D. H.: Proceedings Conference on Magnetism and Magnetic Materials, (AIEE, 1956) , p. 675. Gould, H. L. B., Wenny, D. H.: Elec. Eng., 1957, 76, 208.
[7] Burket, R. E., Stewart, D. M.: J. Appl. Phys., 1962, 33, 1224.
[8] Fahlenbrach, H.: Metall, 1962, 16, 1185.
[9] Bozorth, R. M.: Phys. Rev., 1934, 46, 232.
[10] Becker, R., Doring, W.: Ferromagnetismus, (Verlag-Springer von Jalius, 1939) , 8. 420.
[11] Dahl, O., Pawlek, F.: Z. Physik., 1935, 94, 504.
[12] Bozorth, R. M.: Proceedings Conference on Magnetism and Magnetic Materials, (AIEE, 1956) , p. 69.
[13] Kaya, S.: J. Fac. Sci., Hokkaido Univ., 1938, 2, 29.
[14] Iida, S.: J. Phys. Soc. Japan 1952, 7, 373.
[15] Kaya, S.: Rev. Mod. Phys., 1953, 25, 49.
[16] Chikazumi, S.: J. Phys. Soc. Japan, 1956, 11, 551.
[17] Rathenau, G. W.: 文献[15] 中的讨论, 报导了Snoek & Smit的实验.
[18] Ferguson, E. T.: Compt. Rend., 1957, 244, 2363. Ferguson, E. T.: J. Appl. Phys., 1958, 29, 252.
[19] Snoek, J. L.: Physica, 1939, 6, 161, 797. Snoek, J. L.: Physica, 1941, 8, 711, 734.
[20] Neel, L.: J. Phys. Radium, 1951, 12, 339. Neel, L: J. Phys. Radium, 1952, 13, 249.
[21] Neel, L.: J. Appl. Phys., 1959, 30, 35.
[22] Chikazumi, S.: J. Phys. Soc. Japan, 1950, 5, 327, 333.
[23] Neel, L.: Compt. Rend., 1953, 237, 1468.
[24] Neel, L.: Compt. Rend., 1953, 237, 1613.
[25] Neel, L.: J. Phys. Radium, 1954, 15, 225.
[26] Taniguchi, S., Yamamoto, M.: Sci Rept. Res. Inst. Tohoku Univ., 1954, A6, 330.
[27] Taniguchi, S.: Sci. Rept. Res. Inst. Tohoku Univ., 1955, A7, 269.
[28] Van Vleck, J. H.: Phys. Rev., 1937, 52, 1178.
[29] Takahashi, M., Kono, T.: J. Phys. Soc. Japan, 1960, 15, 936.
[30] Takahashi, M., Kono, T.: J. Phys. Soc. Japan, 1961, 16, 1478.
[31] Graham, C. D.: J. Phys. Soc. Japan 1961, 16, 1481.
[32] Seeger, A.: Z. Metallk., 1953, 44, 247. Seeger, A.: Z. Metallk., 1956, 47, 653.
[33] Sambongi, T., Mitui, T.: J. Phys. Soc. Japan, 1963, 18, 1253.
[34] Heidenreich, R. D., Nesbitt, E. A.: Phys. Rev., 1957, 105. 1678.
[35] Heidenreich, R. D., Nesbitt, E. A., Burbank, R. D.: J. Appl. Phys, 1959, 30, 995.
[36] Nesbitt, E. A., Heidenreich, R. D.: J. Appl. Phys., 1959, 30, 1000.
[37] Nesbitt, E. A., Heidenreich, R. D., Williams, A. J.: J. Appl. Phys., 1960, 31, 228S.
[38] Williams, H. J., Sherwood, R. C.: J. Appl. Phys., 1957, 28, 548.
[39] Graram. C. D.: Magnetic Annealing, Magnetic Properties of Metals and Alloys, (ASM, 1959) , p. 288.
[40] Hart, A.: Brit. J. Appl. Phys., 1960, 11. 58.
[41] Birkenbell, H. J., Cahn, R. W.: J. Appl. Phys., 1961, 32, 3638.
[42] Sixtus, K.: Z. Angew. Phys., 1962, 14, 241.
[43] Neurath, F. W.: J. Appl Phys., 1963, 24, 1315.
[44] Takahashi, M., Sasakawa, T., Fujimori, H.: J. Appl. Phys., 1964, 35, 869.
[45] Adler, E. A.: Z. Angew. Phys., 1963, 15, 250.
[46] Krommuller, H., Seeger, A., Schiller, P.: Z. Naturforsch., 1960, 15a, 740.
No related articles found!
No Suggested Reading articles found!