THE PLASTIC DEFORMATION OF ANTIMONY SINGLE CRYSTALS
BAO SHAN-GER; CHEN NENG-KUAN
Cite this article: 

BAO SHAN-GER; CHEN NENG-KUAN. THE PLASTIC DEFORMATION OF ANTIMONY SINGLE CRYSTALS. Acta Metall Sin, 1964, 7(3): 301-306.

Download:  PDF(1238KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Single crystals of antimony (99.8%) were very brittle at room temperature and twins occurred abundantely during deformation. Their plasticity was improved with increasing temperature and many slip lines were found at 200℃. By means of metallographyic and X-ray methods, it was found that the twinning system is {110} <100> and the slip plane is {111}.
Received:  18 March 1964     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1964/V7/I3/301

[1] Schmid, E., Boas, W.: Plasticity of Crystals, (Hughes, 1950) , p. 94.
[2] Gough, H. J., Cox, H. L.: Proc. Roy. Soc., 1930, A127, 431. Gough, H. J., Cox, H. L.: J. Inst. Metals, 1932, 48, 227. Gough, H. J.: Proc. Am. Soc. Testing Mater., 1933, 33, 3.
[3] Georgieff, M., Schmid, E.: Z. Physik., 1926, 36, 759.
[4] Berg, W. F.: Nature, 1934, 133, 831. Berg, W. F., Sandler, L.: Nature, 1935, 136, 915.
[5] Andrade, E. N. da C.: International Conference on Physics, (Physical Society, London, 1935) , vol. 2, p. 176.
[6] Berg, W. F.: Nature, 1934, 134, 143. Berg, W. F.: International Conference on Physics, (Physical Society, London, 1935) , vol. 2, p. 178.
[7] Gough, H. J., Cox, H. L.: Nature, 1936, 137, 701.
[8] #12
[9] Niggli, P.: Handbuch der Experimental Physik, (Akademle-Verlag GmbH, Berlin, 1928, 7, pt. 1, p. 151.
[10] Hall, E. O.: Twinning and Diffusionless Transformations in Metals, (Butterworths, 1954) , p. 83.
[11] Barrett, C. S.: Cold Working of Metals, (ASM, 1949) , p. 65. Lee, H. T., Brick, R. M.: Trans. Am. Soc. Metals, 1956, 48, 1003.g
No related articles found!
No Suggested Reading articles found!