Abstract  A general review of the strengthening characteristics of the nickel-base superalloys and a primary study of principles of alloying of nickel were described. Three types of strengthening mechanisms of nickel-base alloys: solution-hardening, precipitation-hardening, and grain-boundary hardening, are discussed.
Received:  18 March 1964     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1964/V7/I3/307

[1] Betteridge, W.: The Nimonic Alloys, (Edward Arnold, 1959) .
[2] Ver Snyder, F. L.: High Temperature Materials, Conference Held in Cleveland, Ohio, ed. R. F. Hehemann, (AIME, 1959) , p. 3.
[3] #12
[4] Bieber, C. G., Raudebaugh, R. J.: Precipitation from Solid Solution, (ASM, 1959) , p. 417.
[5] #12
[6] Betteridge, W.: Metallurgia, 1961, 63, 79.
[7] Jahnke, L. P., Frank, R. G.: Metal Progr., 1958, 74, (5) , 77. Jahnke, L. P., Frank, R. G.: Metal Progr., 1958, 74, (6) , 86.
[8] Glenny, E.: Foundary, 1961, 111, 293.
[9] Drennen, D. C., Lund, C. H.: PB, No. 161245, 1961.
[10] #12
[11] Jaffee, R. I.: Progress in Metal Physics, (Pergamon, 1958) , vol. 7, p. 65.
[12] #12
[13] Hansen, M.: Constitution of Binary Alloys, 2nd ed., (McGraw-Hill, 1958) .
[14] #12
[15] #12
[16] Guard, R. W.: Mechanical Behavior of Materials at Elevated Temperatures, (McGraw-Hill, 1961) , p. 270.
[17] Fell, E. A.: Metallurgia, 1961, 63, 157.
[18] Flinn, P. A.: Trans. AIME, 1960, 218, 145.
[19] Guard, R.. W., Westbrook, J. H.: Trans. AIME, 1959, 215, 807.
[20] Radavich, J. F., Pennington, W. J.: Metal Progr., 1961, 79, (2) , 94.
[21] #12
[22] Beattie, Jr., H. J., Ver Snyder, F. L.: Trans. Am. Soc. Metals, 1957, 49, 883.
[23] Kaufman, M.: Trans. AIME, 1963, 227, 405.
[24] Radavich, J. F., Couts, Jr., W. H.: Trans. Am, Soc. Metals, 1961, 54, 591.
[25] Radavich, J. F., Boesch, W. J.: Advance in X-ray Analysis, ed. W. M. Mueller, (Plenum Press, 1960) , vol. 4, p. 233.
[26] Beattie, Jr., H. J.: Acta Cryst., 1958, 11, 607.
[27] #12
[28] #12
[29] #12
[30] #12
[31] #12
[32] McLean, D.: Vancancies and Other Point Defects in Metals and Alloys, (Inst. Metals, 1958) , p. 159.
[33] #12
[34] Schoeck, G.: Mechanical Behavior of Materials at Elevated Temperatures, (McGraw-Hill, 1961) , p. 79.
[35] Cottrell, A. H., Relation of Properties to Microstructure, (ASM, 1954) , p. 330.
[36] Nutting, J., Arrowsmith, J. M.: Structural Processes in Creep, (Iron Steel Inst., 1962) , p. 147.
[37] Mader, S.: Electron Microscopy and Strength of Crystals, (Interscience. 1962) , p. 183.
[38] #12
[39] #12
[40] Fell, E. A., Mitchell, W. I., Wakeman, D. W.: Structural Processes in Creep, (Iron Steel Inst., 1962,), p. 136.
[41] Nordheim, R., Grant, N. J.: Trans. AIME, 1954, 200, 211.
[42] Wilde, R. F., Grant, N. J.: Trans. AIME, 1957, 209, 865.
[43] Kaufman, M., Palty, A. E.: Trans. AIME, 1960, 218, 107.
[44] Hagel, W. C., Beattie, Jr., H. J.: Trans. AIME, 1959, 215, 967.
[45] Rogen, N. E., Grant, N. J.: Trans. AIME, 1960, 218, 180.
[46] Mihalisin, J. R., Decker, R. F.: Trans. AIME, 1960, 218, 507.
[47] #12
[48] #12
[49] Mihalisin, J. R., Carroll, K. G.: Symposium on Advance in Electron Metallography, (ASTM, 1958) , p. 68.
[50] #12
[51] McLean, D.: Met. Rev., 1962, 7, (28) , 481.
[52] Firey, D. N., Freeman, J. W., White, A. E.: NACA TN-No. 2385, 1951.
[53] Mott, N. F., Nabarro, F. R. N.: Conference on Strength of Solid, (Bristal, 1948) , p. 1.
[54] #12
[55] Nicholson, R. B., Nutting, J., Hirsch, P. B.: J. Inst. Metals, 1957-1958, 86, 7.
[56] Dew-Hughes, D., Robertson, W. D.: Acta Met., 1960. 8, 147.
[57] Kelly, A., Fine, M. F.: Acta Met., 1957, 5, 365.
[58] Kelly, A.: Phil. Mag., 1958, 3, 1472.
[59] Orowan, E.: Symposium on Internal Stresses in Metals and Alloys, (Inst. Metals, 1948) , p. 47.
[60] Fischer, J. C., Hart, E. W., Pry, R. H.: Acta Met., 1953, 1, 336.
[61] 张兴钤:合金的強化,全国第一次金属物理学术报告会論文,1961年,沈阳.
[62] Gregory, E., Goetzel, C. G.: Trans. AIME, 1958, 212, 868.
[63] Cremens, W. S., Grant, N. J.: Proc. Am. Soc. Testing Mater., 1958, 58, 714.
[64] Gatti, A.: Powder Met., 1962, (10) , 77.
[65] Schafer, R. J., Quatinetz, M., Weeton, J. W.: Trans. AIME, 1961, 221, 1099.
[66] 师昌緒:高温材料的发展,1963年中国金属学会学术年会論文,青島.
[67] Greenwald, M., Sparrow, W. H.: J. Metals, 1963, 15, 78.
[68] Cottrell, A. H.: Symposium on Creep and Fracture of Metals at High Temperature, (London, 1956) , p. 141.
[69] Glen, J.: J. Iron Steel Inst. (London), 1958, 189, 333.
[70] Hale, K. F.: Vierter Internationaler Kongress fur Electronen Mikroskopie, (Berlin, 1958) , p. 650.
[71] #12
[72] #12
[73] Betteridge, W., Franklin, A. W.: J. Inst. Metals, 1956-1957, 85, 473.
[74] Weaver, C. W.: J. Inst. Metals, 1959-1960, 88, 296.
[75] Fleetwood, M. J.: J. Inst. Metals, 1962, 90, 429.
[76] Weaver, C. W.: J. Inst. Metals, 1962, 90, 404.
[77] #12
[78] McLean, D.: Grain Boundaries in Metals, (Oxford, 1957) , p. 322.
[79] McLean, D.: Mechanical Properties of Metals, (Wiley, 1962) , p. 223.
[80] Cottrell, A. H.: Structural Processes in Creep, (Iron Steel Inst. 1962) , p. 1.
[81] #12
[82] Davies, P. W., Dennison, J. P.: J. Inst. Metals, 1958-1959, 87, 119.
[83] Chang, H. C. (张兴钤), Grant, N. J.: Trans. AIME, 1953, 197, 1175. Chang, H. C. (张兴钤), Grant, N. J.: Trans. AIME, 1956, 206, 544.
[84] Gemmell, G. D., Grant, N. J.: Trans. AIME, 1957, 209, 417.
[85] Resnick, R., Seigle, L.: Trans. AIME, 1957, 209, 87.
[86] Chen, C. W. (陈志文), Machlin, E. S.: Trans. AIME, 1957, 209, 829.
[87] Reid, B. J., Greenwood, J. N.: Trans. AIME, 1958, 212, 503.
[88] Weaver, C. W.: Acta Met., 1960, 8, 343.
[89] Weaver, C. W.: J. Inst. Metals, 1958, 87, 126.
[90] Conrad, H.: Mechanical Behavior of Materials at Elevated Temperatures, (McGraw-Hill, 1961) , p. 218.
[91] Zener, C.: Elasticity and Anelasticity of Metals, (Univ. of Chicago Press, 1948) , p. 158.
[92] Gifkins, R. D.: Acta Met., 1956, 4, 98.
[93] Weaver, C. W.: J. Inst. Metals, 1959-1960, 88, 296.
[94] #12
[95] Pennington, W. J.: Metal Progr., 1958, 73, (3) , 82.
[96] Decker, R. F., Freeman, J. W.: Trans. AIME, 1960, 218, 277.
[97] McLean, D.: J. Inst. Met., 1957, 85, 468.M
No related articles found!
No Suggested Reading articles found!