A STUDY OF THE EQUILIBRIUM BETWEEN HF-H_2O GAS AND SLAGS OF THE CaO-CaF_2 AND CaO-SiO_2-CaF_2 SYSTEM |
HS(?) YUAN-SUN; CHOU YUAN-HSI; LIU FU-LIEN(Institute of Metallurgy; Academia Sinica) |
|
Cite this article:
HS(?) YUAN-SUN; CHOU YUAN-HSI; LIU FU-LIEN(Institute of Metallurgy; Academia Sinica). A STUDY OF THE EQUILIBRIUM BETWEEN HF-H_2O GAS AND SLAGS OF THE CaO-CaF_2 AND CaO-SiO_2-CaF_2 SYSTEM. Acta Metall Sin, 1964, 7(1): 24-31.
|
Abstract An equilibrium study of the reactionCaF_2(in slag)+H_2O=CaO(in slag)+2HF.between HF-H_2O gas and slags of the CaO-CaF_2 and CaO-SiO_2-CaF_2 system has been carried out with a view to evaluating activities in the said slags. Values of the ratioα_(CaO)/α_(CaF_2) are calculated from experimental data, and activities of the individual components are obtained from the α_(CaO)/α_(CaF_2) values with the modified Gibbs-Duhem equations derived by the authors for binary and ternary systems.It has been shown that the simple ratio CaO/SiO_2 can be used as a suitable criterion for the basicity of CaO-SiO_2-CaF_2 slags. The beneficial effects of a fairly basic slag for suppressing silica reduction and fluorine volatilization in blast-furnace smelting of fluorine-bearing iron ore are discussed in the light of the present results.
|
Received: 18 January 1964
|
[1] 周仁、邹元爔、孙鍾礼等:金属学报,1958,3,181. [2] 周仁、邹元爔、徐元森等:金属学报,1958,3,17. [3] 徐元森、邹元爔:化学学报,1963,20,(3) ,181. [4] #12 [5] Baak, T.: Acta Chem. Scand., 1954, 8, 1727. [6] Oelsen, W., Maetz, H.: Mitt. K. Wilh. Inst. Eisenforsch., 1941, 23, 202. [7] Wagner, C.: Thermodynamics of Alloys, (Addison-Wesley, 1952) , p. 18. [8] Baak, T.: The Physical Chemistry of Steelmaking, ed. J. F. Elliott, (Wiley, 1958) , p. 84. [9] Lenfesty, F. A., Brosheer, J. C.: Ind. Eng. Chem., 1952, 44, 1448. [10] Kubaschewski, O., Evans, E. LL.: Metallurgical Thermochemistry, (Academic, 1951) , p. 306. [11] Perrin, R.: Brit. Patent, 1955, Apr., 20, No. 728, 447. [12] 周仁、邹元爔、徐元森等:金属学报,1959,4,1.J |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|