THE SOLUBILITY OF HYDROGEN IN LIQUID IRON, NICKEL, IRON-COPPER AND IRON-COPPER-NICKEL ALLOYS |
YANG WEI-SHEN(Institute of Metal Research; Academia Sinica) |
|
Cite this article:
YANG WEI-SHEN(Institute of Metal Research; Academia Sinica). THE SOLUBILITY OF HYDROGEN IN LIQUID IRON, NICKEL, IRON-COPPER AND IRON-COPPER-NICKEL ALLOYS. Acta Metall Sin, 1964, 7(1): 1-11.
|
Abstract The solubility of hydrogen in molten iron, nickel, iron-copper and iron-copper-nickel alloys has been studied. Methods for solubility determination and deoxidizing conditions of specimens have been examined and comparison of experimental results with thermodynamic calculations shows that insufficient deoxidation of melts may lead to inaccurate results.Experimental results obtained with helium argon and molybdum methods are compared, and the helium method appears to be the most reliable. In the present investigation, all determinations except the hydrogen solubility in nickel were made with the helium method.Addition of copper to molten iron increases the solubility of hydrogen up to 25% Cu, the solubility appears to decrease with further addition. The addition of nickel to liquid Fe-Cu alloys up to 7% Ni has no appteciable effect on the solubility of hydrogen.
|
Received: 18 January 1964
|
[1] Sieverts, A.: Z. Physik. Chem., 1907, 60, 129; 1911, 77, 591. [2] Iwase, K.: Sci. Rept. Res. Inst. Tohoku Univ., 1926, 15, 531. [3] Martin, E.: Arch. Eisenhuttenw., 1929, 407. [4] #12 [5] Liang, H., Bever, B., Floe, F.: Trans. AIME, 1946, 167, 395. [6] #12 [7] #12 [8] Busch, T., Dodd, R. A.: Trans. AIME, 1960, 218, 488. [9] Chipman, J.: I. Iron Steel Inst. (London), 1955, 180, 97. [10] Langenberg, F. C.: Trans. AIME, 1956, 206, 1099. [11] Ohtani, M., Gokcen, N. A.: Trans. AIME, 1960, 218, 533. [12] Floridis, T. P., Chipman, J.: Trans. AIME, 1958, 212, 549. [13] #12 [14] Sieverts, A., Zapf, G., Moritz, H.: Z. Physik. Chem., 1939, 183, 19. [15] #12 [16] #12 [17] Lepp, H.: J. Iron Steel Inst. (London), 1940, 141. 329. [18] Sieverts, A.: Z. Metallk., 1929, 21. 37. [19] Sieverts, A., Hagen, H.: Z. Physik. Chem., 1934, 169, 257. [20] Floridis, T. P., Chipman, J.: Trans. AIME, 1958, 212, 549 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|