Please wait a minute...
Acta Metall Sin  2010, Vol. 46 Issue (2): 179-183    DOI: 10.3724/SP.J.1037.2009.00118
论文 Current Issue | Archive | Adv Search |
ZrO2∶Eu 3+ NANOCRYSTAL FABRICATION AND ITS LUMINESCENCE PROPERTIES BY ION EXCHANGE METHOD
SHA Ren1; WANG Xigui1;LI Xia2
1.Inner Mongolia Key Laboratory for Physics and Chemistry of Functional Materials; College of Chemistry and Environmental Science; Inner Mongolia Normal University; Huhhot 010022
2.College of Rare Earth; Inner Mongolia University of Science and Technology; Baotou 014010
Cite this article: 

SHA Ren WANG Xigui LI Xia. ZrO2∶Eu 3+ NANOCRYSTAL FABRICATION AND ITS LUMINESCENCE PROPERTIES BY ION EXCHANGE METHOD. Acta Metall Sin, 2010, 46(2): 179-183.

Download:  PDF(1609KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Eu3+ doped luminescent nano–materials have become a research focus due to their outstanding physical and chemical properties in light–emitting, magnetism, thermology, catalysis and chemical activity etc.. Furthermore, the relationship between crystal structure and energy levels transition of these nano–materials can be easily obtained by measuring the spectra of doped Eu3+. Among luminescence nano–materials, ZrO2 nano–crystal as a potential one has been attracted great attention in its higher refractive, good optical transparency and relatively low phonon energy. By now certain materials doped RE ion in the matrix ZrO2 for ZrO2∶Er3+–Y3+, ZrO2∶Pr3+ and ZrO2∶(Pr3+, Sm3+) etc., and mesoporous ZrO2 nano–crystals doped Eu3+ by hydrothermal way have been reported. In present study, the ZrO2∶Eu3+ nano–crystal was prepared with high purity and uniform composition by ion exchange method using strong OH− as a precipitant. Its composition, morphology and structure were characterized by XRD, TEM, HRTEM and EDS. The experimental results show that it has a tetragonal crystal structure and its average grain size is 5—20 nm after calcined at 800 ℃ . It is found that the microstructure of ZrO2∶Eu3+ changes slightly with the increase of calcining temperature till a small amount of monoclinic phase forms after calcined at higher than 900  ℃. The luminescent properteof Eu3+ in the ZrO2 nano–crystal were measured by 3D emission and excitation spectra. The characteristic emissin bands of 590 nm (5D0 →7F1) and 606 nm (5D0 →7F2) of Eu3+ were observed at an excitation spectrum of λex=394 nm. The luminescent properties of ZrO2∶Eu 3+ are very sensitive to its microstructure change since slight changes in the ZrO2∶Eu 3+ microstructure cause the changes in the shape and intensity of its emission spectra.

Key words:  ZrO2∶Eu 3+  aocrystal      ion exchange method      luminescence property     
Received:  25 February 2009     
Fund: 

Supported by National Natural Science Foundation of China (No.20161001) and Natural Science Foundation of Inner Mongolia (No.200711020213)

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2009.00118     OR     https://www.ams.org.cn/EN/Y2010/V46/I2/179

[1] Song H W, Chen B J, Peng H S. Appl Phys Lett, 2002; 8: 1776
[2] Park J K, Park S M, Kim C H. J Mater Sci Lett, 2001; 20: 2231
[3] Guo Y F, Ma W M, Wen L, Shen S F, Liu J, Wang H D, Yin K. Acta Metall Sin, 2008; 44: 1149
(郭易芬, 马伟民, 闻 雷, 沈世妃, 刘晶, 王华栋, 伊 凯. 金属学报, 2008; 44: 1149)
[4] Sha R, Wang X G, Wu H Y, Li X. Chin J Inorg Chem, 2008; 24: 981
(莎仁, 王喜贵, 吴红英, 李 霞. 无机化学学报, 2008; 24: 981)
[5] Li P L, Yang Z P, Wang Z J, Xiong Z J, Guo Q L. Acta Phys–Chim Sin, 2008; 24: 179
(李盼来, 杨志平, 王志军, 熊志军, 郭庆林. 物理化学学报, 2008; 24: 179)
[6] Liu G X, Su R X, Wang J X, Dong X T. Chem J Chin Univ, 2008; 29: 461
(刘桂霞, 苏瑞相, 王进贤, 董相廷. 高等学校化学学报, 2008; 29: 461)
[7] Fu S L, Yin T, Ding Q, Zhao W R. Acta Phys Sin, 2006; 55: 4940
(符史流, 尹涛, 丁球, 赵韦人. 物理学报, 2006; 55: 4940)
[8] Jiang S, Schulze W A, Stangle G C. J Mater Res, 1997; 12: 2374
[9] Lu G, .Miura N, Yamazoe N. J Mater Chem, 1997; 7: 1445
[10] Yu Y, Zhou B B. Acta Phys in, 2006; 55: 4332
(俞莹, 周百斌. 物理学报, 2006; 55: 4332)
[11] Liu J X, L  S C, Li X M. Spectrosc Spectral Anal, 2006; 26: 593
(刘金霞, 吕树臣, 李秀明. 光谱学与光谱分析, 2006; 26: 593)
[12] Yang X J, Chen Y H, Shi C S. J Chin Rare Earth Soc, 2002; 20: 531
(杨秀健, 陈永虎, 施朝淑. 中国稀土学报, 2002; 20: 531)
[13] Liu H Q, Wang L L, Zou B S. Acta Phy Sin, 2007; 56: 556
(刘晃清, 王玲玲, 邹炳锁. 物理学报, 2007; 56: 556)
[14] Li X M, Lu S C, Liu J X. Chin J Lumin, 2005; 26: 220
(李秀明, 吕树臣, 刘金霞. 发光学报, 2005; 26: 220)
[15] Chen W, Joly A G, Kowalchuk C M, Malm J, Huang Y. J Phys Chem, 2002; 106B: 7034
[16] Chen L M, Liu Y N, Li Y D. J Alloys Compd, 2004; 381: 266

No related articles found!
No Suggested Reading articles found!