| 高密度脉冲电流对Fe-Si-B非晶合金晶化过程的影响 |
| 晁月盛;滕功清;谢春辉;耿岩;赖祖涵 |
| 东北大学;东北大学理学院 |
|
| EFFECT OF HIGH CURRENT DENSITY LECTROPULSING ON THE CRYSTALLIZATION PROCESS OF AMORPHOUS Fe-Si-B ALLOY |
| CHAO Yuesheng; TENG Gongqing; XIE Chunhui; GENG Yan; LAI Zuhan (Northeastern University; Shenyang 110006) |
引用本文:
晁月盛;滕功清;谢春辉;耿岩;赖祖涵. 高密度脉冲电流对Fe-Si-B非晶合金晶化过程的影响[J]. 金属学报, 1996, 32(11): 1204-1208.
,
,
,
,
.
EFFECT OF HIGH CURRENT DENSITY LECTROPULSING ON THE CRYSTALLIZATION PROCESS OF AMORPHOUS Fe-Si-B ALLOY[J]. Acta Metall Sin, 1996, 32(11): 1204-1208.
| 1卢柯,王景唐,董林.金属学报,1991;27:B312LuK,WangJT,WangWT,WeiWD.JApplPhys,1991;69:5223KosterU,SchunemannU,Blank-BewersdorffM,BrauerS,SuttonM,StephensonGB.MaterSciEng,1991;A133:6114KulikT,HorubataT,MatyjaH.MaterSciEng,1992;A157:1075ChaoYuesheng,LaiZuhan,HeKaiyuan,ErHongru.MaterSciEng,1994;A181//A182:9826TengGQ,ChaoYS,LaiZH,DongL,JMaterSciLett,1995;14:1447KoshimuraM,TakahashiM.In:MasumotoT,SuzukiKeds.,ProcIntConfRapidlyQuenchedMetals.JIM,1982;1:5398KemenyT,VinczeI,FogarrassyB.PhysRev,1979;B20:4769EgamiT,IEEETransMagn,1981;17:260010郑兆勃编著.非晶固体材料引论.北京:科学出版社,1987:19411秦荣山,鄢红春,何冠虎,周本濂.材料研究学报,1995;9:219 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|