| KPO_3-MoO_3熔盐相图 |
| 方建慧;唐赟;李郁;阎立诚;陈念贻;王继扬 |
| 上海大学;上海;201800;上海大学;上海;201800;上海大学;上海;201800;上海大学;上海;201800;上海大学;上海;201800;山东大学;济南;250012 |
|
| KPO_3-M0O_3 PHASE DIAGRAM |
| FANG Jianhui; TANG Yun; LI Yu; YAN Licheng; CHEN Nianyi (Shanghai University;Shanghai 201800); WANG Jiyang (Shandong University; Jinan 250012)(Manuscript received 1996-04-08; in revised form 1996-09-10) |
引用本文:
方建慧;唐赟;李郁;阎立诚;陈念贻;王继扬. KPO_3-MoO_3熔盐相图[J]. 金属学报, 1997, 33(4): 395-397.
,
,
,
,
,
.
KPO_3-M0O_3 PHASE DIAGRAM[J]. Acta Metall Sin, 1997, 33(4): 395-397.
1Bergman A G,Bogotova E I.Zh Neorg Khim,1964;9:2182 2方建慧,陈念贻,阎立诚,王继扬.见:史启祯,陈佩珩,冉新权,唐宗薰,张逢星主编,第八届全国相图学术会议论文集。西安:西北大学,1995:115 3Zigg D S,Makovsty L E,Tischer R E,Brown F R,Hercules M J.J Phys Chem,1980;84:2898 4Bergman A G,Semenyakova L V.Vkr Khim Zh,1971;37:15 |
|