| Fe-Cu-Nb-V-Si-B纳米晶合金磁导率与温度的关系 |
| 王治;何开元;尹君;张玉梅;张洛;梁志德 |
| 东北大学材料科学与工程系;沈阳;110006;天津理工学院材料物理研究所;天津;300191;东北大学材料科学与工程系;沈阳;110006;东北大学材料科学与工程系;沈阳;110006;东北大学材料科学与工程系;沈阳;110006;上海钢铁研究所;上海;200940;东北大学材料科学与工程系;沈阳;110006 |
|
| TEMPERATURE DEPENDENCE OF PERMEABILITY FOR Fe-Cu-Nb-V-Si-B NANOCRYSTALLINE ALLOY |
| WANG Zhi;HE Kaiyuan;YIN Jun;ZHANG Yumei;ZHANG LuO;LIANG Zhide (Department of Material Science and Engineering; Northeastern University; Shenyang 110006)(Institute of Materials Physics; Tianjin Institute of Technology; Tianjin 300191)(Shanghai Iron and Steel Research Institute; Shanghai 200940) |
引用本文:
王治;何开元;尹君;张玉梅;张洛;梁志德. Fe-Cu-Nb-V-Si-B纳米晶合金磁导率与温度的关系[J]. 金属学报, 1998, 34(2): 200-204.
,
,
,
,
,
.
TEMPERATURE DEPENDENCE OF PERMEABILITY FOR Fe-Cu-Nb-V-Si-B NANOCRYSTALLINE ALLOY[J]. Acta Metall Sin, 1998, 34(2): 200-204.
1Yoshisawa Y, Ogums S, Yamauchi K.J Appl phys, 1988; 64: 6044 2Hener G. IEEE Trans Magn, 1989; MAG-25: 3327 3Hernando A, Vazquez M, Kulik T, Prados C. Phys Rev B, 1995; 51: 3581 4Varga L K, Kisdi-Koszo E, Zsoldos E, Bakos E. IEEE Trans Magn, 1994; 30: 552 5Varga L K, Bakos E, Kisdi-Koszo E, Zsoldos E, Kiss L F. J Magn Magn Mater 1994; 131: 280 6Bigot J,Lecaude N,Perron J C,Milan C,Ramiarinjaona C,Rialland J F. J Magn Magn Mater,1994;131:299 7Gawior W, Kolano R,Wojcik N.Mater,Sci Eng,1991;A133:172 8 Baricco M, Antonione C, Allia P, Tiberto P, Vinai F Mater Sci Eng, 1994; A179/A18O: 572 9 Allia P, Baricco M, Knokel M, Tiberto P, Vinai F.J Magn Magn Mater, 1994; 131: 243 10 Wang Z, He K Y, He S L, Zhang Y M, Fu Y J, Zhang L,J Magn Magn Mater,1997; 171: 300 11 Herzer G.Mater,Sci Eng,1991;A133:1 12王治,何开元,张治,金属学报,1997;33:1289 (Wang Z, He K Y, Zhang L. Acta Metall Sci, 1997; 33: 1289) 13王治,何开元,尹君,赵玉华,物理学报, 1997;46:2054(Wang Z,He K Y,Yin J, Zhao Y H. Acta Phys Sic,1997; 46:2054) 14 Wang Z, He K Y, He S L, Zhang L, Jin J, Zhang Y M, Cheng L Z. Accepted by Mater Sci Eng, 1997 |
|