纳米复合磁体磁化过程的计算机研究
初业隆;熊良钺;孙校开
中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015
COMPUTER STUDY OF MAGNETIZATION IN NANOCOMPOSITE MAGNETS
CHU Yelong; XIONG Liangyue; SUN Xiaokai (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)
引用本文:

初业隆;熊良钺;孙校开. 纳米复合磁体磁化过程的计算机研究[J]. 金属学报, 1998, 34(4): 423-430.
, , . COMPUTER STUDY OF MAGNETIZATION IN NANOCOMPOSITE MAGNETS[J]. Acta Metall Sin, 1998, 34(4): 423-430.

全文: PDF(805 KB)  
摘要: 对Nd2Fe14B/α-Fe纳米复合磁体单个粉末颗粒的磁化过程进行了计算机模拟.在不同条件下得到三种磁滞回线,即:Stoner—Wohlfarth型、细腰型和具有良好矩形度的磁滞回线.并且研究了约化剩磁、内禀矫顽力和最大磁能积随晶粒尺寸a和软磁相含量fm的变化.结果表明,对fm=40%的模型复合磁体.a=25nm时最大磁能积达到最大(BH)max=375kJ/m3,比纯Nd—Fe—B模型磁体的(BH)max=264kJ/m3有明显提高.
关键词 纳米复合磁体交换相互作用计算机模拟    
Abstract:The computer simulation of magnetization process of a single powder particle of the Nd2Fe14B/α-Fe nanocomposite magnet has been performed. Three types of hysteresis loops have been observed at different conditions: Stoner-Wohlfarth like type, contracted loop and normal hysteresis loop with a good rectangularity. The behavior of the reduced remanence, the intrinsic coercivity and the change of maximum magnetic energy product with the grain size, a,and the content of the soft phase, fm, have been studied. For the model nanocomposite magnetsof fm=40% and the grain size a=25 nm, the optimum value of (BH)max=375 kJ/m3 is attained.It is remarkably enhanced in comparison with the maximum of (BH.)max=264 kJ/m3 of the pure Nd-Fe-B magnet.
Key wordsnanocomposite magnet    exchanged interaction    computer simulation
收稿日期: 1998-04-18     
基金资助:国家自然科学基金!59571014
1 McCallum R W, Kadin A M, Clemente G B, Keem J E. J Appl Phys, 1987; 61: 3577
2 Manaf A, Buckley R A, Davies H. J Magn Magn Mater, 1993; 128: 302
3 Kneller E P, Hawig R. IEEE bens Magn, 1992; MAG-27: 3588
4 Skomski R, Coey J M D. Phys Rev, 1993; 48B: 15812
5 Schrefl T, Fidler J, Kronmller H. Phys Rev, 1994; 49B: 6100
6 Liu W, Wang Q, Sun X K, Zhao X G, Zhao T, Zhang Z D, Chuang Y C. J Magn Magu Mater, 1994; 131: 413
7 Yang J L, Wang Q, Sun X K, Zeng G Y, Chen M, Liu W, Zhao X G, Zhso T, Zhang Z D. J Mop Magn Maten 1994; 134: 197
8 Jin Z Q, Sun X K, Liu W, Zhao X G, Xiao Q F, Sui Y C, Zhang Z D, Wang Z G, Qin H X. i Magn Magn Mater, 1997; 169: 135
9 Fukunaga H, Inoue H. Jpn J Appl Phgs, 1992; 31: 1347
10 Binder K, Heermann D W 著 秦克诚译. 统计物理学中的蒙特罗模拟方法. 北京:北京大学出版社, 1994: 33 (Binder K, Heermann D W ed, Qin Kecheng trans. Monte Carlo Simulation in Statistical Physics. Beijing:Peking Uni Press, 1994; 33)
11 Zijlstra H. In: Wohlfarth E P ed., Fermmagnetic Materiats, Vol.3., Amsterdam: N0rth-Holland Publishing, 1982: 37
12 Kronmller H. In: Long G J, Grandjcan F eds., Supermaguets, Hard Manetic Materiais, Dordrecht:Kluwer Academic Publisherrs, 1990: 461
13 Chudnovsky E M, In: Fernandez-baca J A, Ching Wai-Yim eds., The Manetism of Amorphous Metais and Alloys. Singapore: World Scientific, 1995: 143
14 Herzer G. IEEE Trans Magn, 1990; MAG-26: 1397
15 Otani Y, Li H S, Coey J M D. IEEE Trans Magn, 1990; MAG-26: 2658
[1] 张林; 徐送宁; 张彩碚; 祁阳 . 熔融Cu55团簇在冷却过程中结构变化的分子动力学模拟[J]. 金属学报, 2008, 44(10): 1161-1166 .
[2] 郑洲顺; 曲选辉; 雷长明 . PIM充模流动过程中粘度的变化与缺陷形成[J]. 金属学报, 2007, 43(2): 183-193 .
[3] 侯华; 赵宇宏; 陈铮; 徐宏 . 相场法预测低铝合金Ni75AlxV25-x的早期沉淀过程[J]. 金属学报, 2005, 41(7): 695-702 .
[4] 张林; 张彩碚; 王元明 . 连续冷却过程中低碳钢奥氏体→铁素体相变的元胞自动机模拟[J]. 金属学报, 2004, 40(1): 8-13 .
[5] 朱明刚; 李卫; 李岫梅; 郭永权 . 纳米复合Nd4.5(Fe, Ga, Co)77.5B18磁体的矫顽力和交换耦合作用[J]. 金属学报, 2003, 39(2): 217-220 .
[6] 李晨曦; 隋智通; 李玉海 . 高Ti炉渣中Ca-Ti矿相析出过程的计算机模拟[J]. 金属学报, 2001, 37(7): 763-766 .
[7] 李殿中; 张玉妥; 刘实; 李依依 . 材料制备工艺的计算机模拟[J]. 金属学报, 2001, 37(5): 449-452 .
[8] 鲁世强; 罗子健; 王仁卉; 曾凡昌 . 合成电子衍射花样的计算机模拟及应用[J]. 金属学报, 1999, 35(5): 554-560 .
[9] 王明章; 李小燕; 林实; 王中光; 肖纪美 . 计算机模拟晶界位向对双晶体循环形变行为的影响[J]. 金属学报, 1999, 35(1): 27-31 .
[10] 隋智通;张培新. 硼渣中硼组分选择性析出行为[J]. 金属学报, 1997, 33(9): 943-951.
[11] 戎咏华;王永瑞;王纪文;陈行康;胡赓祥. 20钢奥氏体氮碳共渗后淬火态与时效态的化合物层[J]. 金属学报, 1996, 32(5): 462-468.
[12] 尹爱君;李晶;李新海;黄克雄;蒋汉瀛. 铜闪速熔炼中微量元素行为的计算机模拟[J]. 金属学报, 1996, 32(4): 387-392.
[13] 陈达. 纳米微晶材料的扩散机制[J]. 金属学报, 1995, 31(8): 340-345.
[14] 徐驰;苏航;陈念贻;李洁;唐定骧. DyF_3-BaF_2-LiF三元系熔体结构的计算机模拟研究[J]. 金属学报, 1995, 31(15): 97-102.
[15] 蔡珣;周平南. 显微硬度实验的计算机模拟[J]. 金属学报, 1995, 31(13): 44-5.