| 任意固相反扩散条件下枝晶凝固溶质传输微观/宏观模型化 |
| 徐达鸣;张成军;司广琚 |
| 哈尔滨工业大学材料科学与工程学院;哈尔滨;150001;佳木斯大学工学院;佳木斯;154007;哈尔滨工业大学材料科学与工程学院;哈尔滨;150001 |
|
| MICRO-/MACRO-SCOPIC MODELING OF SOLUTAL MASS TRANSPORT IN DENDRITE SOLIDIFICAfION WITH PARTIAL SOLID BACK DIFFUSION |
| XU Daming ; ZHANG Chengjun ; SI Guangju (School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001)(Engineering College; Jiamusi University; Jiamusi 154007) |
引用本文:
徐达鸣;张成军;司广琚. 任意固相反扩散条件下枝晶凝固溶质传输微观/宏观模型化[J]. 金属学报, 1998, 34(7): 678-688.
,
,
.
MICRO-/MACRO-SCOPIC MODELING OF SOLUTAL MASS TRANSPORT IN DENDRITE SOLIDIFICAfION WITH PARTIAL SOLID BACK DIFFUSION[J]. Acta Metall Sin, 1998, 34(7): 678-688.
1 Bennon W D, Incropera F P. Int J Heat Mass Transfer 1987; 30: 2161, 2171 2 Prescott P J, Incropera F P, Bennon W D. Int J Heat Maas Transfer, 1991; 34: 2351 3 Voller V R, Prakash C. Int J Heat Mass Transfer 1987; 30: 1709 4 Beckermann C. Viskanta R. Phys Chem Hydrodyn. 1988: 10: 195 5徐达鸣,李庆春,安阁英铸造,1997;(4):44 (Xu Damin., Li Qingchun, An Geying Foundry, 1997(4): 44) 6 Diao Q Z, Tsai H L. Metall Trans, 1993; 24A: 963 7顾江平清华大学博士学位论文,1995(Gu Jiangping.PhD Thesis,Tsinghua University,1995) 8 Rappaz M, Voller V. Metall Trans, 1990; 21A: 749 9 Schneider M C, Beckermann C. Int J Heat Mass Transfer, 1995; 38: 3455 10徐达鸣.哈尔滨工业大学博士学位论文,1989(Xu Daming、PhD Thesis,Harbin Institute of Technology,,1989) 11 Xu Daming, Li Qingchun. Numer Heat Transfer, 1991; 20A: 181; 203 12 Shahani H, Amberg G, Fredriksson H. Metall Trans, 1992; 23A: 2301 13陈卫德.大连理工大学博士学位论文,1994(Chen Weide.PhD Thesis,Dalian University of Science and Engineering,1994) 14徐达鸣,李庆春.金属学报,1990;26:B267(Xu Daming, Li Qingchun. Acta Metall Sin, 1990; 26: B267) 15 Gray W G. Chem Egg Sci, 1975; 30: 229 16 Ni J, Beckermann C. Metall Trans, 1991; 22B: 349 17 Flemings M C, Nereo G E. Trans Metall Soc AIME, 1967; 239: 1449 18 1980; (1): 6(Balangin G F. Cast Product, 1980; (1): 6) 19 Geiger G H, Poirier D R. Transport Phenomena in Metallurgy. Reading, Mass: Addison-Wesley, 1973:20司广琚.哈尔滨工业大学硕士学位论文,1996(Si Guangju.Master Thesis,Harbin Institute of Technology,1996) 21 Bower T F, Brody H D, Flemings M C. Trans Metall Soc AIME, 1966; 236: 624 22 Xu Daming, Si Guanaiu. In: Proc 3rd Pacific Rim Int Conf on Modeling of Casting and SolidificationPriestes 1996, Beijing: International Academic Publishers, 1996: 228 |
|