| Al—Mn合金中粒子促进形核及初期再结晶织构 Ⅱ.粒子与其它形核位置的交互作用及初期再结晶织构 |
| 杨平;O.Enler |
| 德国亚琛工业大学金属研究所;Kopernikusstr.14;D—52056;Aachen;Germany |
|
| PARTICLE STIMULATED NUCLEATION AND THE FORMATION OF RSCRYSTALLIZATION TEXTURE IN Al-Mn ALLOY CONTAINING PARTICLES Ⅱ. Interaction Between Particles and Other Nucleation Sites and the Formation of Recrystallization Texture |
| YANG Ping; O.ENGLER(Institute of Metal Science and Metal Physics; Aachen University of Technology; Kopernikusstr. 14; D-52056;Aachen; Germany) Now: School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing;100083 Now: Los Alamos National Laboratory; Center for Materials Science; K765; Los Alamos; NM87545; USACorrespondent: YANG Ping; Tel: (010)62333436; Fax: (010)62332336 |
引用本文:
杨平;O.Enler. Al—Mn合金中粒子促进形核及初期再结晶织构 Ⅱ.粒子与其它形核位置的交互作用及初期再结晶织构[J]. 金属学报, 1998, 34(8): 793-801.
,
.
PARTICLE STIMULATED NUCLEATION AND THE FORMATION OF RSCRYSTALLIZATION TEXTURE IN Al-Mn ALLOY CONTAINING PARTICLES Ⅱ. Interaction Between Particles and Other Nucleation Sites and the Formation of Recrystallization Texture[J]. Acta Metall Sin, 1998, 34(8): 793-801.
1 Bleck W, Bunge H J. Acta Metall, 1981; 29: 1401 2 rsund R, Nes E. Scr Metall, 1988; 22: 665 3 Juul Jensen D, Hansen N, Humpherys F J. Acta Metall, 1985; 33: 2155 4 Weiland H, Rouns T N, Liu J. Z Metallkd, 1994; 85: 592 5 Humphreys F J, Ferry M, Johnson C, Pailard P. 16th Ris Inter Sym, Ris National Lab., Denmark1995: 87 6 Johnson C P, Humphreys F J. In: Liang Z et al eds., ICOTOM-11, X'ian, China, 1996: 1263 7 Engler O, Yang P, Kong X. Actd Maten 1996; 44: 3349 8 Nes E, In: Hansen N et al eds., 1st Ris Inter Sym Ris National Lab., Denmark, 1980: 85 9 杨平, Engler 金属学报, 1998; 34: 785(Yang P, Engler O. Acta Metall Sin, 1998; 34: 785) 10 Engler O, Escher C, Gottstein G. Textures Mcrostrvct, 1996; 26: 337 11 Yang P, Engler O. In: Hansen N eds., 16th Ris Inter Symp, Ris National Lab., Denmark, 1995: 595 12 Humphreys F J. In: Hansen N ed., 1st Ris Inter Symp, Ris National Lab., Denmark, 1980: 35 13 Humphreys P J. In: Chandra T ed., Recrystallization'90. The Minerals, Metals & Society 1990: 113 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|